Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 21.0 kV/mm @Thickness 2.00 mm |
533 kV/in @Thickness 0.0787 in |
ASTM D149 |
Nilit Nilamid B3 H G8 40% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G8 is a product that combines outstanding strength and stiffness with good moldability and good impact strength. It is widely used for structural applications.Key character.. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 1.60 mm |
533 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Lexan® BFL2000 PC Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 1.60 mm |
533 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Lexan® BFL2000 PC (Asia Pacific) Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 1.60 mm |
533 kV/in @Thickness 0.0630 in |
Short Term; ASTM D149 |
Shell Carilon® DP P1000 Polyketone
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON® Thermoplastic Polymer DP P1000 is the first in a family of developmental engineering polyketone resins fr.. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 2.00 mm |
533 kV/in @Thickness 0.0787 in |
ASTM D149 |
Nilit Nilamid A G5 FR C4 25% Glass Fiber Reinforced, Flame Retardant PA66 (with Halogens) Description: Nilamid A G5 FR C4 combines excellent mechanical performance with flame retardancy. The halogenated flame retardant system used in this product allows a wide range of colors. This produ.. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 2.00 mm |
533 kV/in @Thickness 0.0787 in |
ASTM D149 |
Nilit Nilamid B3 H G6 30% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G6 is a general purpose, 30% glass fiber reinforced NYLON 6 with a combination of good mechanical performance, impact strength and processability. It is one of the most wid.. |
|||
Dielectric Strength | 21.0 - 60.0 kV/mm | 533 - 1520 kV/in | Average value: 31.3 kV/mm Grade Count:20 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
Dielectric Strength | 21.0 - 35.0 kV/mm | 533 - 889 kV/in | Average value: 27.5 kV/mm Grade Count:4 |
Overview of materials for Nylon, Amorphous Transparent Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Amorphous Transparent Alloy". Each property range of values reported is minimum and maximum value.. |
|||
Dielectric Strength | 21.0 kV/mm | 533 kV/in | VDE 0303 |
GEHR Plastics ECTFE Polyethylene Chlorotrifluoroethylene Ethylene-Chlortrifluorethylene exhibits an extraordinary impact strength at temperatures ranging from -76°C to 150°C. A great part of the product properties attributes to the very smooth surfa.. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 1.00 mm |
533 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical LUMID GN1001AF PA6, Halogen Free Flame Retardant Feature: Injection Molding, PA6, Halogen Free Flame RetardantApplication: Electrical & Electronic (Switch)CAS No. 25038-54-4 and 37640-57-6Information provided by LG Chemical |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 1.00 mm |
533 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical LUMID LW4203A(W) PA6+GF/MF20%, Low Warpage Feature: Injection Molding, PA6+GF/MF20%, Low WarpageApplication: Automotive Parts (Engine Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 1.00 mm |
533 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical LUMID LW4403B(W) PA66+GF/MF40%, Low Warpage Feature: Injection Molding, PA66+GF/MF40%, Low WarpageApplication: Automotive PartsCAS No. 32131-17-2, 13983-17-0 and 65997-17-3Information provided by LG Chemical |
|||
Dielectric Strength | 21.0 kV/mm | 533 kV/in | ASTM D149 |
Kolon KOPA® KN333G30CRN G/F Reinforced Nylon 66 Oil resistantApplications Surge tanksInformation provided by API-Kolon. |
|||
Dielectric Strength | 21.0 kV/mm | 533 kV/in | ASTM D149/DIN 53481 |
Kolon KOPA® KN333G33CR G/F Reinforced Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Dielectric Strength | 21.0 kV/mm | 533 kV/in | ASTM D149 |
Kolon KOPA® KN333HB40HFBL Hybrid Nylon 66 High flow, dimensionally stableApplications Fans & ShroudsInformation provided by API-Kolon. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 1.91 mm |
533 kV/in @Thickness 0.0750 in |
|
Momentive Performance Materials TSE3033 Clear General Purpose Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Dielectric Strength | 21.0 kV/mm | 533 kV/in | |
Momentive Performance Materials TSE3940 Flame Retardant Adhesive Sealant, Gray TSE3940 and TSE3941 flame retardant adhesive/sealants are non-flowable, one-component RTVs that cure quickly by reacting with atmospheric moisture forming a soft elastic silicone rubber. These mater.. |
|||
Dielectric Strength | 21.0 kV/mm | 533 kV/in | |
Momentive Performance Materials TSE3940 Gray Adhesive Sealant, Fast Cure Paste One-part totally non-corrosive alkoxy cure. Alkoxy cure silicones are neutral cure materials that offer exceptional adhesion and are non-corrosive to most metals. Typical uses: Flame retardant, no.. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 3.20 mm |
533 kV/in @Thickness 0.126 in |
ASTM D149 |
Solvay Specialty Polymers Amodel® AE-1133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high .. |
|||
Dielectric Strength | 21.0 kV/mm | 533 kV/in | ASTM D149 |
Samyang Tramid® 210G35 Polyamide, Reinforced Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210G35 is a reinforced grade.Applications:Automotive gear level housingConnectors.. |
|||
Dielectric Strength | 21.0 kV/mm | 533 kV/in | ASTM D149 |
Samyang Tribit® 1500G20 PBT, Reinforced General Purpose Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1500G20 is a reinforced, general purpose gr.. |
|||
Dielectric Strength | >= 21.0 kV/mm @Frequency 50.0 Hz |
>= 533 kV/in @Frequency 50.0 Hz |
ASTM D149 |
Borealis LE4212L Polyethylene Insulation Compound, Crosslinkable LE4212L is a natural low-density crosslinkable polyethylene compound. Specifications: IEC 60502-1; and ANSI/ICEA S-66-524.Information provided by Borealis AG |
|||
Dielectric Strength | 21.0 kV/mm | 533 kV/in | ASTM D149-95a |
Thermoseal KLINGERSIL® C-4433 Compressed Inorganic Fiber Sheet Fiberglass, Aramid & Inorganic FibersNitrile BinderUltimate Steam SheetOutstanding Load BearingExcellent Creep RelaxationBest General Purpose SheetInformation provided by Thermoseal Inc. |
|||
Dielectric Strength | 21.0 kV/mm | 533 kV/in | D149 |
Zhejiang Juner 201-G30 30% Glass Fibre Reinforced Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Dielectric Strength | 21.0 kV/mm | 533 kV/in | IEC 60243-1 |
DSM Arnitel® PL581 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Dielectric Strength | 21.0 kV/mm | 533 kV/in | IEC 60243-1 |
DSM Arnitel® PM581 58 Shore D, Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 2.00 mm |
533 kV/in @Thickness 0.0787 in |
ASTM D149 |
Toyobo T-751 Nylon, Painting Grade Key Feature: Glass fiber and mineral reinforced, high heat distortion and impact gradesInformation provided by Toyobo Co., Ltd |
|||
Dielectric Strength | 21.0 - 34.0 kV/mm | 533 - 864 kV/in | Average value: 27.3 kV/mm Grade Count:3 |
Overview of materials for Nylon 66/6, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, Mineral Reinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Dielectric Strength | 21.0 - 39.4 kV/mm | 533 - 1000 kV/in | Average value: 29.0 kV/mm Grade Count:19 |
Overview of materials for PVC, Wire and Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr.. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 2.00 mm |
533 kV/in @Thickness 0.0787 in |
IEC 243-1 |
LATI LARAMID G/45 45% Glass Filled Polyphthalamide (PPA) Based Compound
(Unverified Data**) Laramid compounds are based on a unique semi-crystalline engineering polymer (polyphthalamide) offering improved performance compared to traditional engineering thermoplastics at a lower cost than s.. |