Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Front Barrel Temperature = 316 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Polymer Resources PC-G10-[color]-1 Polycarbonate, 10% Glass Reinforced with Mold Release
Polycarbonate, 10% Glass Reinforced with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Polymer Resources PC-G20-[color]-1 Polycarbonate, 20% Glass Reinforced with Mold Release
Polycarbonate, 20% Glass Reinforced with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Polymer Resources PC-G40 Polycarbonate, 40% Glass Reinforced
Polycarbonate, 40% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p..
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Polymer Resources PC-G40-[color]-1 Polycarbonate, 40% Glass Reinforced with Mold Release
Polycarbonate, 40% Glass Reinforced with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Polymer Resources PC-HM-FR1 Polycarbonate, 10% Glass Reinforced, Flame Retardant
Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Polymer Resources PC-HM-FR1-[color]-4 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold Release
Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig..
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Polymer Resources PC-HM-FR2-[color]-4 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold Release
Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig..
Front Barrel Temperature 316 - 329 °C
601 - 624 °F
Solvay Specialty Polymers Amodel® A-1130 FW Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1130 FW is a 30% glass-fiber reinforced polyphthalamide (PPA) grade containing a solid lubricant. This resin was designed for moderate-pressure, low-velocity friction and wear applications...
Front Barrel Temperature 316 - 329 °C
601 - 624 °F
Solvay Specialty Polymers Amodel® A-1133 NL WH 505 Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1133 NL resin is a 33% glass reinforced polyphthalamide (PPA) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatibilit..
Front Barrel Temperature 316 - 329 °C
601 - 624 °F
Solvay Specialty Polymers Amodel® A-4122 HR WH 117 Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-4122 HR resin is a 22% glass reinforced polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhibits high heat resistance, high st..
Front Barrel Temperature 316 - 329 °C
601 - 624 °F
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0..
Front Barrel Temperature 316 - 329 °C
601 - 624 °F
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi..
Front Barrel Temperature 316 - 329 °C
601 - 624 °F
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi..
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Polymer Resources PC-HM-FR1-[color]-TFE Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear Resistant
Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes..
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
PTS Tristar® PC-10R-(6) 6 MFI Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
LTL Color Compounds ColorFast® PCGF130 Polycarbonate, 30% Glass-Filled
30% glass-filled grade polycarbonateAll information provided by LTL Color Compounders, Inc.
Front Barrel Temperature 316 - 329 °C
601 - 624 °F
Solvay Specialty Polymers Amodel® A-1130 FW Polyphthalamide (PPA), 30% Glass Fiber
Amodel® A-1130 FW is a 30% glass-fiber reinforced polyphthalamide (PPA) grade containing a solid lubricant. This resin was designed for moderate-pressure, low-velocity friction and wear applicati..
Front Barrel Temperature 316 - 324 °C
601 - 615 °F
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Conditioned)
Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in..
Front Barrel Temperature 316 - 329 °C
601 - 624 °F
Solvay Specialty Polymers Amodel® AS-1933 HS Polyphthalamide (PPA), 33% Glass Fiber
Amodel® AS-1933 HS is a 33% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e..
Front Barrel Temperature 316 - 329 °C
601 - 624 °F
Solvay Specialty Polymers Amodel® AT-1001L Polyphthalamide (PPA)
Amodel® AT-1001L is an unreinforced, impact modified polyphthalamide (PPA) resin that exhibits exceptional impact strength at temperatures ranging from room temperature to as low as -40°F (-40..
Front Barrel Temperature 316 - 329 °C
601 - 624 °F
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA), 25% Glass Fiber (Dry)
Amodel® AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s..
Front Barrel Temperature 316 - 343 °C
600 - 650 °F
Star Plastics PCGF10 Molding Grade PC with 10% Glass
Information provided by Star Plastics, Inc.
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Samyang Trirex® PC-3027U 6 MFI UV Stabilized Clear Polycarbonate
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 316 - 329 °C
601 - 624 °F
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Conditioned)
Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist..
Front Barrel Temperature 316 - 329 °C
601 - 624 °F
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist..
Front Barrel Temperature 316 - 329 °C
601 - 624 °F
Solvay Specialty Polymers Amodel® A-1945 HSL Polyphthalamide (PPA)  (discontinued **)
Amodel A-1945 HSL is a 45% glass reinforced grade of polyphthalamide (PPA) resin. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment. Thi..
Front Barrel Temperature 316 - 329 °C
601 - 624 °F
Solvay Specialty Polymers Amodel® AS-1933 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1933 HS is a 33% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material excee..
Front Barrel Temperature 316 - 329 °C
601 - 624 °F
Solvay Specialty Polymers Amodel® AS-1945 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1945 HS is a 45% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material excee..
Front Barrel Temperature 316 - 329 °C
601 - 624 °F
Solvay Specialty Polymers Amodel® AT-1001L Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-1001L is an unreinforced, impact modified polyphthalamide (PPA) resin that exhibits exceptional impact strength at temperatures ranging from room temperature to as low as -40°F (-40°C), ..
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Celanese FORTRON® 1140 E7 Polyphenylene Sulfide (PPS)
Description: Fortron 1140E7 is an inherently flame-retardant grade exhibiting extremely low flash and fast cycle times. It has excellent electrical properties, high hardness and stiffness. This grad..