Shuman 603 Black HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Shuman
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shuman 603 Black HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High density, injection molding grades, good chemical resistance.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density >= 0.952 g/cc
>= 0.0344 lb/in³
ASTM D1505
Melt Flow 2.0 - 3.9 g/10 min
2.0 - 3.9 g/10 min
ASTM D1238
4.0 - 5.9 g/10 min
4.0 - 5.9 g/10 min
6.0 - 9.9 g/10 min
6.0 - 9.9 g/10 min
10 - 14.9 g/10 min
10 - 14.9 g/10 min
15.0 - 18.0 g/10 min
15.0 - 18.0 g/10 min
Processing Properties Metric English Comments
Processing Temperature 182 - 210 °C
360 - 410 °F