Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Processing Temperature = 210 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 160 - 210 °C
320 - 410 °F
Celanese Ateva® 1063 Ethylene Vinyl Acetate Copolymer Film  (discontinued **)
Laminating and coextrusion applications; excellent sealability, opticals, strength, and low COF.
Processing Temperature 190 - 210 °C
374 - 410 °F
Cylinder temp
Asahi Kasei Tenac® 5012 Acetal Homopolymer  (discontinued **)
Standard-flow grade, with reduced stiffness and increased elongation through addition of special polymers.Applications: Clips, fasteners, press-fit parts.This product is not a part of the standard p..
Processing Temperature 180 - 210 °C
356 - 410 °F
Blow molding cylinder temperature
LG Chemical KEYFLEX TO-1088A Thermoplastic Olefin for Injection Molding, 88A Hardness
KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber ..
Processing Temperature 185 - 210 °C
365 - 410 °F
Taiwan Sheen Soon Sheenthane® A8700F Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD.
Processing Temperature 180 - 210 °C
356 - 410 °F
Taiwan Sheen Soon Sheenthane® A9080 Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD.
Processing Temperature 182 - 210 °C
360 - 410 °F
Shuman 603 Black HDPE
High density, injection molding grades, good chemical resistance.Data provided by the manufacturer.
Processing Temperature 195 - 210 °C
383 - 410 °F
Wanhua Chemical Wanthane® WHT-1295B Polyester Based TPU
Good mechanical properties, good extrusion stability, low costInformation provided by Wanhua Chemical Group Co., Ltd.
Processing Temperature 190 - 210 °C
374 - 410 °F
Wanhua Chemical Wanthane® WHT-1495B Polyester Based TPU
Good extrusion stability, high transparency, excellent mechanical propertiesInformation provided by Wanhua Chemical Group Co., Ltd.
Processing Temperature 170 - 210 °C
338 - 410 °F
ELASTO UK Dryflex® 420401S SBS Based Material, 40D Hardness, Natural
The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for..
Processing Temperature 170 - 210 °C
338 - 410 °F
ELASTO UK Dryflex® 422351S SBS Based Material, 35D Hardness, Black
The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for..
Processing Temperature 180 - 210 °C
356 - 410 °F
ELASTO UK Dryflex® 500400S SEBS Based Material, Unfilled Qualities, 40A Hardness, Translucent
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
Processing Temperature 180 - 210 °C
356 - 410 °F
ELASTO UK Dryflex® 500900S SEBS Based Material, Unfilled Qualities, 90A Hardness, Translucent
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
Processing Temperature 180 - 210 °C
356 - 410 °F
ELASTO UK Dryflex® 502500S SEBS Based Material, Unfilled Qualities, 50A Hardness, Black
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
Processing Temperature 193 - 210 °C
379 - 410 °F
stock temperature
Chevron Phillips Marlex® HHM TR-305 Medium density hexene copolymer
Benefits: good processability, excellent melt strength, broad fusion range, outstanding stress cracking resistanceApplications: geomembrane, gas and chemical containment liners, landfill linersInfor..
Processing Temperature 180 - 210 °C
356 - 410 °F
ELASTO UK Dryflex® 600600S SEBS Based Material, Filled Qualities, 60A Hardness, Natural
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material ..
Processing Temperature 193 - 210 °C
379 - 410 °F
stock temperature
Chevron Phillips Marlex® HXB TR-512 Extra high molecular weight polyethylene
Benefits: outstanding impact and creep resistance, excellent ESCR, excellent chemical resistanceCharacteristics: ESCR > 700 at Condition A, at 50°C; ASTM D 1693Applications: 55-gallon drums, indust..
Processing Temperature 180 - 210 °C
356 - 410 °F
ELASTO UK Dryflex® 662300S SEBS Based Material, Semi-Filled Qualities, 30A Hardness, Black
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
Processing Temperature 180 - 210 °C
356 - 410 °F
ELASTO UK Dryflex® 662550S SEBS Based Material, Semi-Filled Qualities, 55A Hardness, Black
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
Processing Temperature 180 - 210 °C
356 - 410 °F
ELASTO UK Dryflex® 662650S SEBS Based Material, Semi-Filled Qualities, 65A Hardness, Black
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
Processing Temperature 194 - 210 °C
381 - 410 °F
Optimum Extrusion Conditions
DSM Biomedical Elasthane™ 55D Thermoplastic Polyether Polyurethane (TPU)
A high tensile strength, aromatic biomedical polymer with an exceptional combination of mechanical properties plus biological compatibility Elasthane™ TPU exhibits outstanding hydrolytic stabilit..
Processing Temperature 190 - 210 °C
374 - 410 °F
hot runner
Celanese Celcon® GC25TF POM, 25% Glass Reinforced
Celcon« GC25TF is a 25% glass coupled acetal copolymer formulated for higher flow in thin walled and small parts. Celcon GC25TF is also exceptionally resistant to fuel. It offers excellent resista..
Processing Temperature 190 - 210 °C
374 - 410 °F
hot runner
Celanese Hostaform® C 9021 K POM, Tribological
Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese
Processing Temperature 190 - 210 °C
374 - 410 °F
hot runner
Celanese Hostaform® MR130ACS POM, Specialty
Hostaform« acetal copolymer grade MR130ACS is a general purpose acetal with improved acid stabilization. Hostaform« MR130ACS demonstrates improved performance over standard acetals after intermit..
Processing Temperature 160 - 210 °C
320 - 410 °F
RTP Company RTP 1200-55D  Polyurethane Thermoplastic Elastomer (TPU) 55 Shore D  (discontinu
55 Shore DComments:55-D DurometerUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for th..
Processing Temperature 190 - 210 °C
374 - 410 °F
hot runner
Celanese Hostaform® C 13031 XAP POM, Unfilled
Polyacetal copolymer, reduced emissionInformation provided by Celanese
Processing Temperature 190 - 210 °C
374 - 410 °F
hot runner
Celanese Hostaform® C 27021 LS colored POM, UV Resistant
Information provided by Celanese
Processing Temperature 190 - 210 °C
374 - 410 °F
hot runner
Celanese Hostaform® C 9021 AW POM, Tribological
Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese
Processing Temperature 190 - 210 °C
374 - 410 °F
hot runner
Celanese Hostaform® C 9021 GV3/20 POM, 20% Glass Reinforced
Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese
Processing Temperature 160 - 210 °C
320 - 410 °F
RTP Company RTP 1205-65D  Polyurethane Thermoplastic Elastomer (TPU) Glass Fiber 30% - 65 Shore D &am
Glass Fiber 30% - 65 Shore DComments:Glass Fiber65-D DurometerUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provid..
Processing Temperature 190 - 210 °C
374 - 410 °F
hot runner
Celanese Celcon® GC25T POM, 25% Glass Reinforced
Celcon« GC25T is a 25% glass fiber coupled acetal copolymer grade. It offers higher strength than the standard Celcon GC25-A. Celcon GC25T is FDA approved. Celcon GC25T is also exceptionally resis..
Copyright © lookpolymers.com All Rights Reserved