Polymer Property : Melt Flow = 3.9 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 2.0 - 3.9 g/10 min
2.0 - 3.9 g/10 min
ASTM D1238
Shuman 603 Black HDPE
High density, injection molding grades, good chemical resistance.Data provided by the manufacturer.