Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 180 - 210 °C | 356 - 410 °F | Blow molding cylinder temperature |
LG Chemical KEYFLEX TO-1175A Thermoplastic Olefin for Extrusion, 75A Hardness KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber .. |
|||
Processing Temperature | 170 - 210 °C | 338 - 410 °F | |
ELASTO UK Dryflex® 402901S SBS Based Material, 90A Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Processing Temperature | 170 - 210 °C | 338 - 410 °F | |
ELASTO UK Dryflex® 420451S SBS Based Material, 45D Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Processing Temperature | 170 - 210 °C | 338 - 410 °F | |
ELASTO UK Dryflex® 422401S SBS Based Material, 40D Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Processing Temperature | 180 - 210 °C | 356 - 410 °F | |
ELASTO UK Dryflex® 500500S SEBS Based Material, Unfilled Qualities, 50A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Processing Temperature | 180 - 210 °C | 356 - 410 °F | |
ELASTO UK Dryflex® 500700S SEBS Based Material, Unfilled Qualities, 70A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Processing Temperature | 180 - 210 °C | 356 - 410 °F | |
ELASTO UK Dryflex® 500750S SEBS Based Material, Unfilled Qualities, 75A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Processing Temperature | 180 - 210 °C | 356 - 410 °F | |
ELASTO UK Dryflex® 500900S SEBS Based Material, Unfilled Qualities, 90A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Processing Temperature | 180 - 210 °C | 356 - 410 °F | |
ELASTO UK Dryflex® 600600S SEBS Based Material, Filled Qualities, 60A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Processing Temperature | 180 - 210 °C | 356 - 410 °F | |
ELASTO UK Dryflex® 600650S SEBS Based Material, Filled Qualities, 65A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Processing Temperature | 193 - 210 °C | 379 - 410 °F | stock temperature |
Chevron Phillips Marlex® HXB TR-512 Extra high molecular weight polyethylene Benefits: outstanding impact and creep resistance, excellent ESCR, excellent chemical resistanceCharacteristics: ESCR > 700 at Condition A, at 50°C; ASTM D 1693Applications: 55-gallon drums, indust.. |
|||
Processing Temperature | 180 - 210 °C | 356 - 410 °F | |
ELASTO UK Dryflex® 602350S SEBS Based Material, Filled Qualities, 35A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Processing Temperature | 180 - 210 °C | 356 - 410 °F | |
ELASTO UK Dryflex® 602550S SEBS Based Material, Filled Qualities, 55A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Processing Temperature | 180 - 210 °C | 356 - 410 °F | |
ELASTO UK Dryflex® 602800S SEBS Based Material, Filled Qualities, 80A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Processing Temperature | 180 - 210 °C | 356 - 410 °F | |
ELASTO UK Dryflex® 662900S SEBS Based Material, Semi-Filled Qualities, 90A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Processing Temperature | 190 - 210 °C | 374 - 410 °F | Optimum Extrusion Conditions |
DSM Biomedical CarboSil® 20 80A Thermoplastic Silicone Polycarbonate Polyurethane (TSPCU) A ground-breaking copolymer that combines the biocompatibility and biostability of conventional silicone elastomers with the processability and toughness of thermoplastic polycarbonate-urethanes Th.. |
|||
Processing Temperature | 194 - 210 °C | 381 - 410 °F | Optimum Extrusion Conditions |
DSM Biomedical Elasthane™ 55D Thermoplastic Polyether Polyurethane (TPU) A high tensile strength, aromatic biomedical polymer with an exceptional combination of mechanical properties plus biological compatibility
Elasthane™ TPU exhibits outstanding hydrolytic stabilit.. |
|||
Processing Temperature | 170 - 210 °C | 338 - 410 °F | |
Eurotec® Tecoform® PO20 NL IL POM, impact modified, natural Information provided by Eurotec® |
|||
Processing Temperature | 180 - 210 °C | 356 - 410 °F | |
ELASTO UK Dryflex® 600450S SEBS Based Material, Filled Qualities, 45A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Processing Temperature | 205 - 210 °C | 401 - 410 °F | Injection |
Alliance Polymers Zythane™ 4085A Thermoplastic Polyurethane Elastomer Zythane™ 4085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Processing Temperature | 190 - 210 °C | 374 - 410 °F | hot runner |
Celanese Celcon® GB10 POM, 10% Glass Reinforced Celcon« GB10 is a 10% glass bead filled grade for low shrinkage and warp resistance in large, flat, and thin walled parts.Information provided by Celanese |
|||
Processing Temperature | 190 - 210 °C | 374 - 410 °F | hot runner |
Celanese Celcon® GB25 POM, 25% Glass Reinforced Celcon« GB25 acetal copolymer is a 25% glass bead filled grade for low shrinkage and warp resistance in large, flat and thin walled parts.Information provided by Celanese |
|||
Processing Temperature | 190 - 210 °C | 374 - 410 °F | hot runner |
Celanese Hostaform® C 2521 POM, Unfilled Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese |
|||
Processing Temperature | 190 - 210 °C | 374 - 410 °F | hot runner |
Celanese Hostaform® C 2521 XAP² ™ LS colored POM, UV Resistant POM copolymerInformation provided by Celanese |
|||
Processing Temperature | 190 - 210 °C | 374 - 410 °F | hot runner |
Celanese Hostaform® C 52021 POM, Unfilled Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese |
|||
Processing Temperature | 190 - 210 °C | 374 - 410 °F | hot runner |
Celanese Hostaform® EC140XF POM, Specialty Hostaform« EC140XF is a conductive ESD grade of acetal copolymer for applications requiring dissipation of static build-up. EC140XF has an improved resistance to aggressive fuel blends.Informatio.. |
|||
Processing Temperature | 190 - 210 °C | 374 - 410 °F | hot runner |
Celanese Hostaform® MR130HPB POM, Specialty Preliminary Data SheetInformation provided by Celanese |
|||
Processing Temperature | 190 - 210 °C | 374 - 410 °F | hot runner |
Celanese Hostaform® XGC15-LW01 POM, 15% Glass Reinforced Hostaform« XGC15-LW01 is an injection molding grade reinforced with approx. 15% glass fibers and tribological modification for sliding applications requiring low friction and wear.Information provi.. |
|||
Processing Temperature | 190 - 210 °C | 374 - 410 °F | hot runner |
Celanese Hostaform® C 9021 GV1/20 XGM POM, 20% Tribological Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese |
|||
Processing Temperature | 190 - 210 °C | 374 - 410 °F | hot runner |
Celanese Hostaform® MT8U05 POM, Medical Technology Hostaform« acetal copolymer grade MT8U05 is a special grade developed for medical industry applications containing low residual monomers and no animal products. The material can be identified by U.. |