Fainplast Compounds GS 0145/R Flexible PVC, Injection Molding, Lead Free

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Fainplast Compounds
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds GS 0145/R Flexible PVC, Injection Molding, Lead Free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Technical items with rubber/PU
Physical Properties Metric English Comments
Density 1.17 - 1.21 g/cc
0.0423 - 0.0437 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 62 - 66
62 - 66
ISO R 868
Tensile Strength at Break 11.0 MPa
1600 psi
ISO R 527
Elongation at Break 380 %
380 %
ISO R 527