Samyang Trirex® PC-3025U 12 MFI UV Stabilized Clear Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, UV Stabilized
Manufacturer Samyang
Trade Name Trirex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samyang Trirex® PC-3025U 12 MFI UV Stabilized Clear Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Water Absorption 0.15 %
0.15 %
24 hours at 73°F
Melt Flow 12 g/10 min

@Load 1.20 kg,
Temperature 300 °C
12 g/10 min

@Load 2.65 lb,
Temperature 572 °F
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 62.1 MPa

@Thickness 3.17 mm
9010 psi

@Thickness 0.125 in
Elongation at Break 120 %

@Thickness 3.17 mm
120 %

@Thickness 0.125 in
Flexural Yield Strength 89.6 MPa

@Thickness 3.17 mm
13000 psi

@Thickness 0.125 in
Flexural Modulus 2.21 GPa

@Thickness 3.17 mm
321 ksi

@Thickness 0.125 in
Izod Impact, Notched 7.47 J/cm

@Thickness 3.17 mm
14.0 ft-lb/in

@Thickness 0.125 in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 135 °C
275 °F
ASTM D648
Flammability, UL94 V-2

@Thickness 1.59 mm
V-2

@Thickness 0.0625 in
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Clear grade, but transmission not quantified.
Processing Properties Metric English Comments
Rear Barrel Temperature 254 - 274 °C
490 - 525 °F
Middle Barrel Temperature 266 - 277 °C
510 - 530 °F
Front Barrel Temperature 277 - 293 °C
530 - 560 °F
Nozzle Temperature 271 - 293 °C
520 - 560 °F
Melt Temperature 277 - 293 °C
530 - 560 °F
Mold Temperature 71.1 - 93.3 °C
160 - 200 °F
Drying Temperature 121 °C
250 °F
Dry Time 3 - 4 hour
3 - 4 hour
Injection Pressure 75.8 - 124 MPa
11000 - 18000 psi
Back Pressure 0.345 - 1.38 MPa
50.0 - 200 psi
Clamp Pressure 27.6 - 68.9 MPa
4000 - 10000 psi
Cycle Time - Injection 1.0 - 2.5 sec
1.0 - 2.5 sec
Cycle Time - Cooling 5.0 - 40 sec
5.0 - 40 sec
Vent Depth 0.00200 - 0.00800 cm
0.000787 - 0.00315 in
Screw Speed 40 - 70 rpm
40 - 70 rpm
Descriptive Properties Value Comments
Injection Speed- Edge Gate Slow-Medium
Injection Speed- Tab Gate Medium-Fast
Injection Speed- Tunnel Gate Fast
Shot Size 40-60%