Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 271 - 293 °C | 520 - 560 °F | |
PTS Tristar® PC-10R-(14) 14 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 271 - 293 °C | 520 - 560 °F | |
PTS Tristar® PC-10FR 12 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 271 - 293 °C | 520 - 560 °F | |
PTS Tristar® PC-10FR-(V) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 271 - 293 °C | 520 - 560 °F | |
PTS Tristar® PC-10FR-(VIM) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 271 - 293 °C | 520 - 560 °F | |
PTS Tristar® PC-10FRNH 12 MFI Non-Bromine Non-Chlorine Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 271 - 293 °C | 520 - 560 °F | |
MRC Polymers EMAREXâ„¢ 300 GF43 Nylon 6, 43% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Nozzle Temperature | 277 - 293 °C | 530 - 560 °F | |
MRC Polymers NAXELLâ„¢ PC110-919 General Purpose Polycarbonate, Medium High MFR Polycarbonate for colorable productsMFR can be modified between 10 to 40 g/10minCan be UV stabilizedInternal and external lubricant can be addedCan be clear to color matchedNot for products that req.. |
|||
Nozzle Temperature | 282 - 293 °C | 540 - 560 °F | |
MRC Polymers NAXELLâ„¢ PC429HHI Polycarbonate, Impact Modified, High MFR, EZ Flow Good Property RetentionHeat and Dimensional StabilityHigh Melt Impact ModifiedMFR can be modified between 10 to 26 g/10minsCan be UV stabilizedGenerally for natural, colorable and can go blackIntern.. |
|||
Nozzle Temperature | 266 - 293 °C | 510 - 560 °F | |
Wellman EcoLon® MRGF1518-BK Mineral/Glass Fiber Reinforced Nylon 66, Lubricated, Heat Stabilized, PCR Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Nozzle Temperature | 266 - 293 °C | 510 - 560 °F | |
Wellman Wellamid® 220-N Unfilled Nylon 66, Not Lubricated, Nucleated, or Heat Stabilized Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae.. |
|||
Nozzle Temperature | 266 - 293 °C | 510 - 560 °F | |
Wellman Wellamid® 22LHI3 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Nozzle Temperature | 266 - 293 °C | 510 - 560 °F | |
Wellman Wellamid® 22LHI4 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Nozzle Temperature | 266 - 293 °C | 510 - 560 °F | |
Wellman Wellamid® 22LHI6 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Nozzle Temperature | 266 - 293 °C | 510 - 560 °F | |
Wellman Wellamid® 22LN2-N Unfilled Nylon 66, Lubricated & Nucleated Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae.. |
|||
Nozzle Temperature | 227 - 293 °C | 440 - 560 °F | |
Wellman Wellamid® 42LH XE-N Unfilled Nylon 6, Lubricated & Heat Stabilized Typical Applications: Automotive seat belt, buckle and anchor components; convoluted tubing for wire harnesses; furniture hardware, curtain glides.Data provided by the manufacturer, Wellman Inc. |
|||
Nozzle Temperature | 282 - 293 °C | 540 - 560 °F | |
Wellman Wellamid® MR259 22LH-N 25% Mineral Reinforced Nylon 66, Lubricated & Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Nozzle Temperature | 282 - 293 °C | 540 - 560 °F | |
Wellman Wellamid® MR409 22H-N 40% Mineral Reinforced Nylon 66, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Nozzle Temperature | 254 - 293 °C | 490 - 560 °F | |
Wellman Wellamid® MR410 42H-N 40% Mineral Reinforced Nylon 6, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Nozzle Temperature | 266 - 293 °C | 510 - 560 °F | |
Wellman Wellamid® MRGF3822-BK 38% Mineral/10% Glass Fiber Reinforced Nylon 66, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Nozzle Temperature | 260 - 293 °C | 500 - 560 °F | |
Wellman Wellamid® NY1599-N Unfilled Nylon 66 Description: Unfilled Nylon 66Information provided by Wellman. |
|||
Nozzle Temperature | 254 - 293 °C | 490 - 560 °F | |
Wellman Wellamid® T-731E-BK 10% Reinforced Abrasion Resistant Nylon 6 Description: Abrasion Resistant Nylon 6Information provided by Wellman. |
|||
Nozzle Temperature | 266 - 293 °C | 510 - 560 °F | |
Wellman Wellamid® XT1482-BK High Impact Nylon 66 Description: High Impact Nylon 66Information provided by Wellman. |
|||
Nozzle Temperature | 266 - 293 °C | 510 - 560 °F | |
Wellman Wellamid® XT1482-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Nozzle Temperature | 266 - 293 °C | 510 - 560 °F | |
Wellman Wellamid® XT1486-BK Medium Impact Nylon 66 Description: Medium Impact Nylon 66Information provided by Wellman. |
|||
Nozzle Temperature | 266 - 293 °C | 510 - 560 °F | |
Wellman Wellamid® XT1486-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Nozzle Temperature | 266 - 293 °C | 510 - 560 °F | |
Clariant 6602-L BK-02 Nylon 66, Lubricated, Nucleated, Weather Resistant, Black Data provided by Clariant Masterbatches |
|||
Nozzle Temperature | 266 - 293 °C | 510 - 560 °F | |
Clariant 6604-HSL Nylon 66, Impact Modified, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Nozzle Temperature | 266 - 293 °C | 510 - 560 °F | |
Clariant Renol BRU0000BN-182 Nylon 66, Lubricated, Nucleated, Weather Resistant Data provided by Clariant Masterbatches |
|||
Nozzle Temperature | 266 - 293 °C | 510 - 560 °F | |
Clariant Renol PA611D40 Nylon 612, Glass Fiber Reinforced, Molybdenum Disulfide Lubricated Data provided by Clariant Masterbatches |
|||
Nozzle Temperature | 227 - 293 °C | 440 - 560 °F | Average value: 254 °C Grade Count:5 |
Overview of materials for Nylon 6, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate.. |