Processing Properties | Metric | English | Comments |
---|---|---|---|
Cycle Time - Injection | 1.0 - 2.5 sec | 1.0 - 2.5 sec | |
Samyang Trirex® PC-3020HF 22 MFI Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Cycle Time - Injection | 1.0 - 2.5 sec | 1.0 - 2.5 sec | |
Samyang Trirex® PC-3020U 22 MFI UV Stabilized Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Cycle Time - Injection | 1.0 - 2.5 sec | 1.0 - 2.5 sec | |
Samyang Trirex® PC-3022IR 15 MFI Clear Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Cycle Time - Injection | 1.0 - 2.5 sec | 1.0 - 2.5 sec | |
Samyang Trirex® PC-3022U 15 MFI UV Stabilized Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Cycle Time - Injection | 1.0 - 2.5 sec | 1.0 - 2.5 sec | |
Samyang Trirex® PC-3025IR 10 MFI Clear Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Cycle Time - Injection | 1.0 - 2.5 sec | 1.0 - 2.5 sec | |
Samyang Trirex® PC-3025N2 10 MFI Flame Retardant Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Cycle Time - Injection | 1.0 - 2.5 sec | 1.0 - 2.5 sec | |
Samyang Trirex® PC-3025U 12 MFI UV Stabilized Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Cycle Time - Injection | 1.0 - 2.5 sec | 1.0 - 2.5 sec | |
Samyang Trirex® PC-3027U 6 MFI UV Stabilized Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Cycle Time - Injection | 1.0 sec | 1.0 sec | |
Aaron Industries AAROPRENE® ATPR ECATPR2040 Black Thermoplastic SEBS Rubber AAROPRENE® ATPR 2000 Series Elastomeric CompoundFeatures: A black, thermoplastic SEBS Rubber compound specifically designed for the injection molding of industrial gaskets. |