Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 7.47 J/cm @Temperature 23.0 °C |
14.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® 151R PC Lexan 151R resin is a high viscosicty, nonhalogenated resin designed to be a candidate for applications produced via extrusion or blow molding processing.This data was supplied by SABIC-IP for the A.. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 153R PC (Asia Pacific) Nonhalogenated. 2.5 MFR. Blowmolding/extrusion. UV-stabilized. Internal mold release. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent .. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXD121R PC Transparent/translucent PC for light diffusion special effects. MFR of 18.2. Color package may affect performance. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXE121R PC Transparent PC. ILLUMINATE special effects (fluorescent/edge glow colors). MFR 18.2. Internal mold release. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.17 mm |
14.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Tristar® PC-06R 6.0 MFI Grade Polycarbonate, With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.17 mm |
14.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Tristar® PC-10R-CL(V22) 22 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 7.47 J/cm @Temperature 23.0 °C |
14.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® OQ4620 PC Optical grade with UV cut-off up to 400 nm, greater optical purity than standard grades. For needs of sunglass and sunvisor markets.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 7.47 J/cm @Temperature 22.8 °C |
14.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-BR1-[color]-5 Polycarbonate, Branched, Food Contact Polycarbonate, Branched for Extrusion and Blow MoldingFeatures: • Ultra High Impact Resistance • Ultra High Viscosity • Food Contact AcceptableProcess: Extrusion/Blow MoldingNotes: All physica.. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.17 mm |
14.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Tristar® PC-08 8 MFI Extrusion Grade Polycarbonate Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | 73°F, 0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hybrid B2025IU Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | Lengthwise; ASTM D256 |
G-10 Fiberglass Epoxy Laminate Sheet This glass-epoxy laminate is specified for its extremely high strength and high dimensional stability over temperature. G-10 is used for terminal boards, high humidity applications, electrical and e.. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
M. Holland Company PC522R Polycarbonate High flowHigh impact resistanceGood mold releaseApplications: AppliancesFood containersTable products |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
Global PC-FR2 UL Recognized 94V-2 Polycarbonate Information provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
14.0 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
0.25 mm notch; ASTM D256 |
LG Chemical Lupoy 1200-22 Polycarbonate Resin Description: LUPOY PC 1200-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
14.0 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
0.25 mm notch; ASTM D256 |
LG Chemical Lupoy 1303EP-22 Polycarbonate Resin Description: LUPOY PC 1303EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Izod Impact, Notched | 7.48 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
14.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Lucent Polymers PC-1403FD Polycarbonate, FDA Compliant, Extrusion/Blow Molding Grade Medium FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
14.0 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
0.25 mm notch; ASTM D256 |
LG Chemical Lupoy 1302HP-21 Polycarbonate Resin Description: LUPOY PC 1302HP-21 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Izod Impact, Notched | >= 7.45 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 14.0 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GP1000SW PC, Transparent Description: Injection Molding, PC, General Purpose, TransparencyApplication: Keypad for Mobile Phone, Automotive (Interior)CAS: 103598-77-2Information provided by LG Chemical |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM Data |
Styron CALIBRE™ 200 22 Polycarbonate, General Purpose CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins .. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | 0.125 in; 10 mil notch; ASTM D256 |
Styron CALIBREâ„¢ 201-22 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.17 mm |
14.0 ft-lb/in @Thickness 0.125 in |
|
Samyang Trirex® PC-3025IR 10 MFI Clear Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.17 mm |
14.0 ft-lb/in @Thickness 0.125 in |
|
Samyang Trirex® PC-3025U 12 MFI UV Stabilized Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.17 mm |
14.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Elastoblend® PA6/ABS 1120 B1 Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | 0.125 in; 10 mil notch; ASTM D256 |
Styron CALIBREâ„¢ 303 EP Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.17 mm |
14.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers PC 2109E UV Natural - Extrusion Grade, UV Stabilized, Flame Retardant Polycarbonate Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.17 mm |
14.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers PC 2109T Natural, UV Stabilized, Flame Retardant Polycarbonate Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |