Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX2201 resin uses non chlorinated, non brominated FR additives to deliver a UL94 V1 rating at 1.5 mm. Noryl CRX2201 may be an excellent material candidate where flame resistance and dimensional stability are required.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D 792
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.020 %
0.020 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.020 %

@Temperature 23.0 °C
0.020 %

@Temperature 73.4 °F
ISO 62
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm

@Thickness 3.20 mm
0.0030 - 0.0050 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 6.0 g/10 min

@Load 5.00 kg,
Temperature 280 °C
6.0 g/10 min

@Load 11.0 lb,
Temperature 536 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
8.0 g/10 min

@Load 5.00 kg,
Temperature 280 °C
8.0 g/10 min

@Load 11.0 lb,
Temperature 536 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 63.0 MPa
9140 psi
5 mm/min; ISO 527
76.0 MPa
11000 psi
Type I, 5 mm/min; ASTM D 638
Tensile Strength, Yield 63.0 MPa
9140 psi
5 mm/min; ISO 527
76.0 MPa
11000 psi
Type I, 5 mm/min; ASTM D 638
Elongation at Break 2.8 %
2.8 %
5 mm/min; ISO 527
4.0 %
4.0 %
Type I, 5 mm/min; ASTM D 638
Elongation at Yield 2.8 %
2.8 %
5 mm/min; ISO 527
4.0 %
4.0 %
Type I, 5 mm/min; ASTM D 638
Tensile Modulus 5.50 GPa
798 ksi
1 mm/min; ISO 527
5.60 GPa
812 ksi
5 mm/min; ASTM D 638
Flexural Yield Strength 119 MPa
17300 psi
1.3 mm/min, 50 mm span; ASTM D 790
120 MPa
17400 psi
2 mm/min; ISO 178
Flexural Modulus 5.50 GPa
798 ksi
1.3 mm/min, 50 mm span; ASTM D 790
6.10 GPa
885 ksi
2 mm/min; ISO 178
Izod Impact, Notched 0.260 J/cm

@Temperature -30.0 °C
0.487 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
0.320 J/cm

@Temperature 23.0 °C
0.599 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Notched (ISO) 2.00 kJ/m²

@Temperature -30.0 °C
0.952 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
2.00 kJ/m²

@Temperature 23.0 °C
0.952 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 0.100 J/cm²

@Temperature 23.0 °C
0.476 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
Impact Test 3.00 J

@Temperature 23.0 °C
2.21 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
34.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
18.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow 54.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
30.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
60.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 112 °C
234 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
108 °C

@Thickness 3.20 mm
226 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Vicat Softening Point 124 °C
255 °F
Rate B/50; ASTM D 1525
124 °C
255 °F
Rate B/50; ISO 306
127 °C
261 °F
Rate B/120; ISO 306
Flammability, UL94 V-1

@Thickness 1.50 mm
V-1

@Thickness 0.0591 in
UL 94
Electrical Properties Metric English Comments
Surface Resistance 5.00e+16 ohm
5.00e+16 ohm
ASTM D 257
Dielectric Constant 2.9

@Frequency 50.0 - 60.0 Hz
2.9

@Frequency 50.0 - 60.0 Hz
ASTM D 150
Dielectric Strength 27.0 kV/mm

@Thickness 3.20 mm
686 kV/in

@Thickness 0.126 in
in oil; ASTM D 149
Dissipation Factor 0.0070

@Frequency 50.0 - 60.0 Hz
0.0070

@Frequency 50.0 - 60.0 Hz
ASTM D 150
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved