Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 124 °C | 255 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior... |
|||
Vicat Softening Point | 124 °C | 255 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS (Europe-Africa-Middle East) Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior... |
|||
Vicat Softening Point | 124 °C | 255 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® LG9000 PC+ABS (Europe-Africa-Middle East) CYCOLOY LG9000 is a low gloss PC+ABS injection moulding grade. LG9000 combines good impact / heat and UV resistance with a low gloss surface appearence. It is suitable for automotive interior applic.. |
|||
Vicat Softening Point | 124 °C | 255 °F | ASTM D1525 |
NOVA Chemicals Novapol® HE-Y449-A HDPE Extrusion Resin Features: High ESCR, good toughness, good chemical resistance, good processability.Applications: Pipe coatings, profile extrusions, sheet extrusion for thermoforming, corrugated tubing, conduit.Data.. |
|||
Vicat Softening Point | 124 °C | 255 °F | ASTM D1525 |
NOVA Chemicals Sclair® 2807 HDPE Injection Molding Resin Features: Excellent processability for applications requiring moderate stiffness and toughness, good cold temperature impact properties.Applications: Industrial and lubricant pails.Data provided by .. |
|||
Vicat Softening Point | 124 °C | 255 °F | ASTM D1525 |
Petromont 2001 High Density Polyethylene Resin Petromont HDPE 2001 is a high-density polyethylene copolymer resin produced using the UNIPOL ® Process. This resin has been designed specifically for film for various applications such as notion an.. |
|||
Vicat Softening Point | 124 °C | 255 °F | ASTM D1525 |
SABIC B5429/B5429A High Density Polyethylene for Blow Molding Product Description: B5429 Series grades are medium molecular weight High Density Polyethylene copolymer. They are primarily intended for blow molding articles of small sizes. B5429 series grades.. |
|||
Vicat Softening Point | 124 °C | 255 °F | ASTM D1525 |
Chevron Phillips Marlex® CL-200YJN (Natural) Rotational molding crosslinkable high density polyethylene
(disc Benefits: crosslinks during molding - has outstanding melt strength at 204°C, is formulated to provide maximum UV protection for long-term outdoor weathering, contains an internal mold release, exc.. |
|||
Vicat Softening Point | 124 °C | 255 °F | ASTM D1525 |
Chevron Phillips Marlex® 9506H High Performance Series HDPE Blow Molding Resin
(discontinued **) Resin Type: linear copolymerCharacteristics: superior physical properties, medium molecular weight distribution, wide range of processing conditions, low parison sag, excellent stress crack resistan.. |
|||
Vicat Softening Point | 124 °C | 255 °F | ASTM D1525 |
Reliance Industries Relene E41003 Polyethylene Relene E41003 is a High Density Polyethylene grade with broad molecular weight distribution and good melt strength , suitable for making pipes for water supply, irrigation, sewage and industrial eff.. |
|||
Vicat Softening Point | 124 °C | 255 °F | ASTM D1525 |
Global B-8200 High Density Polyethylene Description-high molecular weight, excellent stress cracking resistance,
excellent impact strength to blow moldApplications-large drums, gasoline tanks, agricultural chemical tanksInformation provi.. |
|||
Vicat Softening Point | 124 °C | 255 °F | ASTM D1525 |
Global J-2208 High Density Polyethylene Description-industrial injection grade w/ UV stabilizer, good for high impact
strengthApplications-high quality industrial products, outdoor applications such as pallets & cratesInformation provided.. |
|||
Vicat Softening Point | 124 °C | 255 °F | ASTM 1525 B10 |
Metabolix Mirel™ F1005 Injection Molding Grade PHA Bioplastic Mirel F1005 is FDA cleared for use in non-alcoholic food contact applications, from frozen food storage and microwave reheating to boiling water up to 212°F. FDA clearance includes products such.. |
|||
Vicat Softening Point | 124 °C | 255 °F | ASTM 1525 B10 |
Metabolix Mirelâ„¢ P1003 Injection Molding Grade PHA Bioplastic Mirelâ„¢ P1003 is a general purpose injection molding material with high modulus.Mirel is suitable for a wide range of injection molded food service and packaging applications including caps and .. |
|||
Vicat Softening Point | 124 °C | 255 °F | ASTM D1525 |
Micropol Isoplas P501 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
Vicat Softening Point | 124 °C | 255 °F | ASTM D1525 |
LyondellBasell Alathon® H5112 High Density Polyethylene, Injection Molding Grade ALATHON H5112 is a medium-molecular-weight-distribution resin with balanced impact/ESCR and high flow characteristics. Typical applications include housewares, food containers, pail handles and toys.. |
|||
Vicat Softening Point | 124 °C | 255 °F | resin; ASTM D1525 |
Lotte Chemical Titan TITANZEX® HI2000 High density polyethylene HI2000 is a high density polyethylene for injection molding. HI2000 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3.2a. A.. |
|||
Vicat Softening Point | 124 °C | 255 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL PVX516 PPE PREVEX* PVX516 resin is a high flow, non FR grade, 110 C HDT |
|||
Vicat Softening Point | 124 °C | 255 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Xylex FXY391DF PC+POLYESTER (Asia Pacific) PC+Polyester alloy in Diffusion Visual fx. This grade is compliant with US FDA/European food contact regulations. Color package may influence performance.This data was supplied by SABIC-IP for the A.. |
|||
Vicat Softening Point | 124 °C | 255 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xylex X7529 PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical quality. UV 400nm block.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Vicat Softening Point | 124 °C | 255 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX.. |
|||
Vicat Softening Point | 124 °C | 255 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS (Asia Pacific) Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX.. |
|||
Vicat Softening Point | 124 °C | 255 °F | ASTM D3417 |
Total HDPE 46060 UV High Density Polyethylene - Large Part Blow Molding Resin Polyethylene: High molecular weight, high density large part blow molding resin.Characteristics:Good melt strengthGood impact and creep resistanceExcellent stress cracking resistanceExcellent stack.. |
|||
Vicat Softening Point | 124 °C | 255 °F | ISO 306 |
Borealis FS1470 High Density Polyethylene FS1470 is a high density polyethylene film grade which combine excellent extrusion behavior with superior mechanical properties. Films made of FS1470 have high impact and tensile strength, and bala.. |
|||
Vicat Softening Point | 124 °C | 255 °F | |
Dow HDPE 65053N High Density Polyethylene DOW HDPE 65053N resin is a narrow molecular weight distribution copolymer designed to offer good environmental stress crack resistance and rigidity with high impact strength. This resin has excellen.. |
|||
Vicat Softening Point | 124 °C @Load 1.02 kg |
255 °F @Load 2.25 lb |
ASTM-D1525 |
Braskem GM5010T2 HDPE High Density Extrusion Polyethylene GM5010T2 is a high-density polyethylene compound specially developed for the manufacturing of extruded pipes. It is produced with bimodal technology and has high molar mass. It shows high mechanical.. |
|||
Vicat Softening Point | 124 °C | 255 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS (Europe-Africa-Middle East) Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX.. |
|||
Vicat Softening Point | 124 °C | 255 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xylex X7529OQ PC+POLYESTER (Asia Pacific) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical qualityThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 124 °C | 255 °F | ASTM D1525 |
ExxonMobil Paxon™ AA50-002 Blow Molding Resin
(discontinued **) AA50-002 is a blow molding grade high density polyethylene. This resin has excellent stress crack resistance combined with high impact strength, rigidity, and melt strength.Information provided by .. |
|||
Vicat Softening Point | 124 °C | 255 °F | ASTM D 1525 |
Total XT10 N Natural HDPE, pipe Applications: Potable water, industrial and mining, sewer and sewer relining, gas and oil gathering, general pipe relining, pipe coatingInformation provided provided by Total Petrochemicals.Total Pe.. |