Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 76.0 MPa | 11000 psi | ASTM D638 |
Nylene® Norpex® AX300 PPE (Polyphenylene Ether); Premium Performance High Heat Properties for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | ASTM D638 |
SABIC Innovative Plastics LNP COLORCOMP PX99848 PA 6 LNP* COLORCOMP* PX99848 is an unfilled Nylon 6 resin. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP FARADEX DX92079 PC (Europe-Africa-Middle East) LNP* Faradex* DX92079 is a compound based on Polycarbonate resin containing Glass Fiber, Glass Bead, Stainless Steel Fiber. Added features of this material include: EMI/RFI Shielding, Mold Release... |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | ASTM D638 |
Solvay Specialty Polymers Amodel® ET-1001 L Polyphthalamide (PPA) Resin, Dry as Molded
(discontinued **) AMODEL ET-1001 L resin is an impact modified polyphthalamide (PPA) with exceptional impact strength and practical toughness. AMODEL PPA resins offer high fatigue strength, and good chemical resistan.. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® 12-032
(discontinued **) PRE-ELEC 12-032 is a conductive thermoplastic compound based on a polyacetal copolymer with 20% carbon fiber. PRE-ELEC 12-032 exhibits excellent mechanical properties and electrical conductivity. Te.. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | 50 mm/min |
Arkema Group Oroglas® MI-4T Acrylic, Heat Resistant
(discontinued **) OROGLAS MI-4T is an acrylic grade that associates improved impact resistance with high heat resistance.Key features improved impact resistance: up to 4 times more impact resistant than standard acr.. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DFL12 PC LNP* Lubricomp* DFL12 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 5% PTFE. Added features include: Internally Lubricated. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PX9406P PPE NORYL* PX9406P resin is an FR (non-halogenated) grade potentially suitable for a variety of electronics applications. RTI (impact) = 105 C. F1 listed in BK color. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PX9406P PPE NORYL* PX9406P resin is an FR (non-halogenated) grade potentially suitable for a variety of electronics applications. RTI (impact) = 105 C. F1 listed in BK color. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP HFG25Z PA 11 LNP* Lubricomp* HFG25Z is a compound based on Nylon 11 resin containing 25% Glass Fiber, 10% Graphite. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP HFG25Z PA 11 (Asia Pacific) LNP* Lubricomp* HFG25Z is a compound based on Nylon 11 resin containing Glass Fiber, Graphite Powder. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP LL002 PEEK LNP* LUBRICOMP* LL002 is a compound based on Polyetheretherketone containing 10% PTFE. Added feature of this material is: Wear Resistant. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | 2 in/min; ASTM Test |
Styrolution Terblend® N NG-04 20% Glass Filled ABS/PA6 (Dry) Terblend N NG-04 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, low mold shrinkage and high heat resistance.Information provided by STYROLUTION, which is a joint ven.. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP WF002 PBT LNP* THERMOCOMP* WF002 is a compound based on PBT containing 10% Glass Fiber. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a.. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS (Asia Pacific) Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a.. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | ISO 527 |
Polyram PlusTek PA340S4 Nylon 66 for Injection Molding, 20% Glass-Beads Reinforced 20% Glass-beads reinforced Nylon 66 for injection molding applications.Information provided by Polyram. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | ASTM D638 |
Washington Penn H2GF3 Polypropylene, 30% Glass Fiber Reinforced Homopolymer. Excellent heat aged physical properties.Applications: Under hood applications, battery trays, exercise equipmentData provided by Washington Penn Plastic Co., Inc. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | Elastic Limit |
Wolf Kunststoff ZEDEX® ZX-324V2T A3F PEEK, PTFE Modified Reduced friction; High wear resistance; High elasticity; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automotive Technology; Machine ToolsInformation provided by Zedex |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | D638 |
Zhejiang Juner 301-G10 10% Glass Fibre Reinforced and Flammable Resistant Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | ISO 527-1/-2 |
Covestro Apec® 2095 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=203 °CPreprocessingMax. Water content |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | |
Covestro Makroblend® UT-620 G Polycarbonate + Polyester Blend Key Features:Contains FillerHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 Septembe.. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | ASTM D638 |
Diamond Polymers NYLON 6 Natural Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | ASTM Data |
Dow Tyril® 880B SAN TYRIL® 880B SAN copolymer combines the high levels of chemical resistance, heat resistance and overall strength of 880 resin with improved mold flow and mold release characteristics.Data provided b.. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | ISO 527 |
Azoty Tarnow™ TARNOFORM 300 GF2 POM 10% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | 50 mm/min |
Arkema Group Cristamid® MS 1300 Semi-Aromatic Nylon (PASA) (Dry) Designation ISO 1874-PA12/xx,MR,12-020Semi-aromatic polyamide (PASA) grade for injection molding and tubes extrusion.Transparency even thick. High resistance to environmental stress cracking. Good t.. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | dry; ISO 527-1/-2 |
Murtfeldt Murylat® SP Polyethylene Terephthalate Murylat® SP combines the properties of Murylat® with improved wear and friction characteristics. It also has increased dynamic resilience which, for example, significantly reduces the required dri.. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | 50% RH; ISO 527-1/-2 |
Murtfeldt Murylat® SP Polyethylene Terephthalate Murylat® SP combines the properties of Murylat® with improved wear and friction characteristics. It also has increased dynamic resilience which, for example, significantly reduces the required dri.. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | ASTM D638 |
Custom Resins Norpex® 300 PPE (Polyphenylene Ether)
(discontinued **) Premium performance high heat. Properties for dry as molded samples.Data provided by the manufacturer |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | v = 50 mm/min; ISO 527-2 |
CENTROPLAST CENTRO HPM Polyphenylensulfone This plastic has very good mechanical, electrical and thermal properties. It has very good hydrolysis resistance, and is suitable for medical, and pharmaceutical equipment construction.Information .. |