Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 8.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Versollan™ OM 1255NX-1 Thermoplastic Elastomer (TPE) Versollan™ OM 1255NX-1 is a high performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS, PC/ABS and copolyester substrates. - Improved Grip with Matte, Rubbery Finish.. |
|||
Melt Flow | 8.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
8.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Eraclene® FA 706 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion Eraclene FA 706 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Films manufactured with Eraclene FA 706 show good processability t.. |
|||
Melt Flow | 8.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
8.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® G360 ABS (Europe-Africa-Middle East) CYCOLAC G360 is a high flow, high impact, medium to high heat resistant injection moulding ABS grade. It is recommended for large or complex parts in the automotive or electrical power tool segments.. |
|||
Melt Flow | 8.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
8.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® G366 ABS (Europe-Africa-Middle East) CYCOLAC G366 is a "new technology" grade of ABS exhibiting outstanding property balance, a good flow, medium impact, medium to high heat resistant and an excellent stability during injection mouldin.. |
|||
Melt Flow | 8.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
8.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycolac® G366 ABS (Europe-Africa-Middle East) CYCOLAC G366 is a "new technology" grade of ABS exhibiting outstanding property balance, a good flow, medium impact, medium to high heat resistant and an excellent stability during injection mouldin.. |
|||
Melt Flow | 8.0 g/10 min @Load 2.16 kg, Temperature 260 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS (Europe-Africa-Middle East) High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra.. |
|||
Melt Flow | 8.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers SAN 300 Natural Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |
|||
Melt Flow | 8.0 g/10 min @Load 2.16 kg, Temperature 260 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS (Europe-Africa-Middle East) UV stabilized, non-FR PC/ABS of excellent flow and impact performanceThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 8.0 g/10 min @Load 3.80 kg, Temperature 260 °C |
8.0 g/10 min @Load 8.38 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® C1110 PC+ABS (Asia Pacific) High impact and ductility at 73F (23C) and -20F (-29C). |
|||
Melt Flow | 8.0 g/10 min @Load 5.00 kg, Temperature 260 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Geloy CR7520 ASA (Europe-Africa-Middle East) Geloy CR7520 is a general purpose injection moulding grade, blend of ASA/SAN. It can be positioned for outside parts in various markets, such as telecommunication, transportation, B&C, lighting and .. |
|||
Melt Flow | 8.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
8.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
LG Chemical HIPS 65IHE PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: Refrigerator Tray, Food Tray, Refrigerator Door LinerCAS: 9003-55-8Information provided by LG Chemical |
|||
Melt Flow | 8.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 (G) |
LG Chemical HIPS MI730 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Melt Flow | 8.0 g/10 min @Load 5.00 kg, Temperature 280 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D 1238 |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Europe-Africa-Middle East) Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
Melt Flow | 8.0 g/10 min @Load 5.00 kg, Temperature 360 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem AUT230M PEI Transparent polyetherimide (Tg 247 degC). Contains low level of mold release. Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are .. |
|||
Melt Flow | 8.0 g/10 min @Load 5.00 kg, Temperature 250 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 482 °F |
ISO 1133 |
SABIC Innovative Plastics Xenoy® 1731 PBT+PC Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD. |
|||
Melt Flow | 8.0 g/10 min @Load 5.00 kg, Temperature 250 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 482 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Xenoy® 1731J PBT+PC (Asia Pacific) PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 8.0 g/10 min @Load 5.00 kg, Temperature 250 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 482 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Xenoy® 1731J PBT+PC (Europe-Africa-Middle East) PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 8.0 g/10 min @Load 5.00 kg, Temperature 250 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 482 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Xenoy® X3108UV PBT+PC (Europe-Africa-Middle East) Unreinforced, UV-stabilized, flame retardant, impact modified PBT+PC with V0 at 0.8mm thickness. For interior and exterior applications like wall switches and electrical enclosures.This data was sup.. |
|||
Melt Flow | 8.0 g/10 min @Load 2.16 kg, Temperature 265 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 509 °F |
ASTM D 1238 |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Asia Pacific) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 8.0 g/10 min @Load 2.16 kg, Temperature 265 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 509 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Xylex X7503HP PC+POLYESTER (Europe-Africa-Middle East) Clear PC-Siloxane copolymer + Polyester alloy, USA Food ContactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 8.0 g/10 min @Load 5.00 kg, Temperature 260 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® HN-3104 PC, 10% Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 8.0 g/10 min @Load 5.00 kg, Temperature 260 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® HN-3104 PC, 10% Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 8.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
8.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM Test |
Styrolution Terluran® HI-10 ABS Terluran HI-10 is an injection molding and extrusion grade of ABS with very high toughness and medium flow.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Melt Flow | 8.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
8.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Styron Magnumâ„¢ 8391 MED Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ MED ABS combines an excellent glossy appearance with high flow and medium impact performance. The mass (continuous process) ABS technology of Styron ensures an ABS resin that .. |
|||
Melt Flow | 8.0 g/10 min @Load 2.16 kg, Temperature 250 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
SABIC Innovative Plastics Valox® SHF4960 PBT (Europe-Africa-Middle East) Valox Super high flow grade, 30% glass filled Flame retardant, High CTI, heat stabilized with mold release. |
|||
Melt Flow | 8.0 g/10 min @Load 5.00 kg, Temperature 250 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 482 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Xenoy® 1731A PBT+PC (Asia Pacific) PBT+PC, Good Impact , Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 8.0 g/10 min @Load 5.00 kg, Temperature 280 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 536 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Noryl MX5569 PPE+PS PPE+PS blend. High Heat. Good balance of flow and impact. Offers good aging performance under heat. Typical applications include Automotive Interiors and Lighting.This data was supplied by SABIC-.. |
|||
Melt Flow | 8.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers SAN 330 BEADS Styrene Acrylonitrile, Transparent Engineering Thermoplastic, High Flow Natural Beads Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 8.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 11008 PVDF Copolymer
(discontinued **) Key features of this grade: Low Viscosity, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVD.. |
|||
Melt Flow | 8.0 g/10 min @Load 5.00 kg, Temperature 260 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Geloy FXW710SK ASA/SAN (Europe-Africa-Middle East) GELOY FXW710SK is an ASA/SAN injection moulding grade. It is suitable for those applications that require sparkle colour effects.This data was supplied by SABIC-IP for the Europe-Africa-Middle East .. |