Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Parallel to Flow = 17.8 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP FARADEX NX07330 PC+ABS (Asia Pacific)
Faradex NX07330 is a compound based on PC+ABS blend resin containing stainless steel and glass fiber. Added features of this material include EMI/RFI Shielding and ESD.
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature -40.0 - 150 °C
17.8 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM 2312EPR PEI
30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature 23.0 - 150 °C
17.8 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM 2312EPR PEI
30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature -40.0 - 150 °C
17.8 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM 2312EPR PEI (Asia Pacific)
30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature 23.0 - 150 °C
17.8 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM 2312EPR PEI (Asia Pacific)
30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature -40.0 - 150 °C
17.8 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics Ultem 2312EPR PEI (Europe-Africa-Middle East)
30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu..
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature 23.0 - 150 °C
17.8 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Ultem 2312EPR PEI (Europe-Africa-Middle East)
30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu..
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS
Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX..
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS (Asia Pacific)
Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX..
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS (Europe-Africa-Middle East)
Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX..
Copyright © lookpolymers.com All Rights Reserved