Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C | 226 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Cycoloy® C1200HFM PC+ABS (Asia Pacific) PC+ABS-MAGIX version in various metallic colors. High heat/good flow characteristics. Appliances, automotive/telecommunication. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C | 226 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYblend 85VB PC/ABS-Blend, Flame Retardant Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C @Thickness 3.20 mm |
226 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C | 226 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C | 226 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Cycoloy® FXC813SK PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC813SK is a multi purpose PC+ABS injection moulding grade, providing a favourable balance of engineering properties. CYCOLOY FXC813SK is suitable for those applications that require sparkl.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C @Thickness 3.20 mm |
226 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS (Asia Pacific) PC+ ABS Automotive applications |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C | 226 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Cycoloy® FXC810MA PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC810MA is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require marble colour effects. The colour package may effect performance.This data was suppl.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C @Thickness 3.17 mm |
226 °F @Thickness 0.125 in |
ASTM D648 |
Metton LMR M1534 Liquid Molding Resin Different product numbers represent different formulations for customer specific needs such as liquid freezing point. Metton LMR is a tough and durable engineering plastic material used to produce .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C @Thickness 6.40 mm |
226 °F @Thickness 0.252 in |
ASTM D648 |
Kingfa MAC-501DY Modified PC/ABS Alloy Features:Excellent balance propertiesGood low temperature impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile license platePower toolComp.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C @Thickness 6.40 mm |
226 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical LUPOY GN5001EF PC/ABS, Br, Cal-free flame retardant Description: Injection Molding, PC/ABS, Halogen Free Flame RetardantApplication: Industrial / IT productCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C @Thickness 3.20 mm |
226 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP NXCY620 PC+ABS LNP* LUBRICOMP* NXCY620 is a compound based on Cycoloy* XCY620 containing Silicone. Added feature of this material is: Lubricant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C | 226 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® PEI 04008 MB Availability: North AmericaForms: PelletsFeatures: Conductive and CopolymerInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C | 226 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics XYLEX HX7509HP PC+POLYESTER Medium flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), fo.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C | 226 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics XYLEX HX7509HP PC+POLYESTER (Europe-Africa-Middle East) Medium flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), fo.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C | 226 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics XYLEX X7509HP PC+POLYESTER (Asia Pacific) PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which r.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C | 226 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP KB008 Acetal Copolymer LNP THERMOCOMP* KB008 is a compound based on Acetal Copolymer resin containing 40% Glass Bead. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C | 226 °F | ISO 75 |
Teijin Multilon DN-1530B Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy Halogen-free flame retardant PC/ABS polymer alloy, and is also antimony-free. It has improved stiffness through the addition of 30 % filler. Improved stiffness and high fluidity realizes a thin wall.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C @Thickness 6.40 mm |
226 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Infino® AE-2130 PC/PET, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C @Thickness 3.20 mm |
226 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Thermotuf U1000AIS PPA LNP* Thermotuf* U1000AIS is a compound based on Polyphthalamide resin. Added features of this material include: High Impact, Heat Stabilized.This data was supplied by SABIC-IP for the Americas regi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C @Thickness 3.20 mm |
226 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL N1150 PPE+PS Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C @Thickness 3.20 mm |
226 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer LNP* STAT-KON* KD000 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C @Thickness 3.20 mm |
226 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON OE006 PPS - Linear LNP* STAT-KON* OE006 is a compound based on PPS - Linear resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C @Thickness 3.20 mm |
226 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOTUF MF004AI PP LNP* Thermotuf* MF004AI is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C @Thickness 3.20 mm |
226 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL BN9003G PPE+HIPS PPE+PS blend. Unfilled. Blow molding. Excellent balance of impact and surface aesthetics. Suitable for automotive exterior components including spoilers. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C @Thickness 3.20 mm |
226 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS (Asia Pacific) Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C @Thickness 3.20 mm |
226 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL N1150 PPE+PS (Europe-Africa-Middle East) Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C | 226 °F | |
Covestro Bayblend® T 84 Polycarbonate/ABS Blend Easier flowing than BAYBLEND T 85 MN.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C | 226 °F | ISO 75-1,-2 |
Covestro Makroblend® UT305 PC/PET Blend Main characteristics:• High toughness even at low temperatures• Good chemical resistance• Good paintability• Good flowability• Low moisture intakeGrade characteristics:• High moisture en.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C @Thickness 3.20 mm |
226 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® ML1661 PC Copolymer (Asia Pacific) Medium-flow impact-modified light-shielding high-flow-ductile PC copolymer. Available in white color only. |