Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS (Europe-Africa-Middle East) Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes.. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer (Europe-Africa-Middle East) This product will be phased out per January 2015 -- Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer (Europe-Africa-Middle East) This product will be phased out per January 2015 -- Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® DMX9254 PC (Asia Pacific) Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl.. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Asia Pacific) Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HPH4704 PPC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® HPS6 PC (Europe-Africa-Middle East) Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer (Europe-Africa-Middle East) XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® XHT4141 PC Copolymer (Europe-Africa-Middle East) XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® 143X PC Copolymer (Asia Pacific) Improved flow PC with excellent processability and mold release. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Europe-Africa-Middle East) Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® HP6NR PC (Asia Pacific) Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® ML5472 PC Gamma sterilization resistant. High heat (PPC). Available in natural color only. Internal mold release.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer (Europe-Africa-Middle East) XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl V01505 PPE+HIPS Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL V01525 PPE+HIPS (Europe-Africa-Middle East) Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature 23.0 - 150 °C |
33.3 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2210K PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature -40.0 - 150 °C |
33.3 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2210K PEI (Asia Pacific) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature -40.0 - 150 °C |
33.3 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem DT1810E PEI Blend (Asia Pacific) Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacifi.. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature -40.0 - 150 °C |
33.3 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM EXUM0169 PEI Blend Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem HATX100 PEI+PCE Higher impact, high flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem HATX100 PEI+PCE (Asia Pacific) Higher impact, high flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem HATX100 PEI+PCE (Europe-Africa-Middle East) Higher impact, high flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature 23.0 - 150 °C |
33.3 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM HU2100 PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. For medical devices and pharmaceutical applications.Healthcare management of change, biocom.. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature -40.0 - 60.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 140 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX987 PPE+PA66 (Asia Pacific) Conductive GTX, CTE 7 |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature 23.0 - 150 °C |
33.3 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL HH180 PPE+PS Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-LOY WF306C PBT (Asia Pacific) LNP* Stat-loy* WF306C is a compound based on Polybutylene Terephalate resin containing Glass Fiber. Added features of this material include: Antistat, Clean Compounding System. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 123X PC Copolymer (Asia Pacific) Improved flow PC with excellent processability and mold release. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS (Europe-Africa-Middle East) Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX.. |