Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 127 °C | 261 °F | ISO 306/A50 |
Premix Thermoplastics PRE-ELEC® PE 1296 Conductive Thermoplastic Compound PRE-ELEC® PE 1296 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1296 has a high concentration o.. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS (Europe-Africa-Middle East) UV stabilized, non-FR PC/ABS of excellent flow and impact performanceThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX7720 PC+ABS (Asia Pacific) Cycoloy resin CX7720 is a non brominated and non chlorinated flame retardant PC/ABS resin grade featuring high heat resistance and thin wall FR. It is UL-94 listed at 1.2 mm V0 and 1.5mm 5VB. Its hi.. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS (Europe-Africa-Middle East) High impact PC+ABS material designed for local Pacific Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS (Europe-Africa-Middle East) PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Asia Pacific) PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS (Asia Pacific) PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525B |
SABIC PP681K Polypropylene Random Copolymer for Injection Molding Product Description: PP 681K is specially developed for producing injection molded articles with high clarity and also has better impact properties than homo PP counterparts.PP 681K has the followi.. |
|||
Vicat Softening Point | 127 °C @Load 5.001 kg |
261 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH GF5030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Vicat Softening Point | 127 °C | 261 °F | 50°C/hr; 50N |
Polimeri Europa KOBLEND PCA 839F PC+ABS
(discontinued **) Symbol according to ISO 1043/1: PC+ABSUnfilled. Suitable for Injection Molding. Supplied as pellets.ISO data. Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses... |
|||
Vicat Softening Point | 127 °C | 261 °F | 50°C/hr; 50N |
Polimeri Europa KOBLEND PCA PD 54 PC+ABS
(discontinued **) Symbol according to ISO 1043/1: PC+ABS Injection moulding grade with flame retardant properties ( UL 94 V-0 at 1.6mm thickness ) and good light resistance. Main application fields: business machin.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
Chevron Phillips HiD® 9354 HDPE Natural Pipe Resin
(discontinued **) Resin Type: gas phase linear hexane copolymerApplications: corrugated pipe applicationsInformation provided by Chevron Phillips Chemical Company. |
|||
Vicat Softening Point | 127 °C | 261 °F | ISO 306 |
Total Finathene® 53140 HDPE, blow molding, sheet
(discontinued **) Finathene® 53140 is a high density polyethylene produced by the slurry loop low pressure polymerization process FINATHENE® 53140 has been especially developed for the manufacturing of blow molded .. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B; ISO 306 |
Covestro Bayblend® 2773 Polycarbonate + ABS Blend, Automotive
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
LyondellBasell Alathon® L5332CP High Density Polyethylene ApplicationsALATHON L 5332CP, formerly known as LYHD 048, is designed to meet the requirements of AAHTO M294 stress crack resistance. It exhibits excellent processing stability and high crush resis.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
LyondellBasell Alathon® M5372 High Density Polyethylene ApplicationsALATHON M 5372 copolymer with narrow weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processing stability. .. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
LyondellBasell Petrothene® LR734045 High Density Polyethylene (Sheet & Profile Extrusion) ApplicationsThe PETROTHENE LR 7340 series of polyethylene resins exhibits good stiffness and ESCR. Typical applications include bottles for household chemicals.Regulatory StatusThe base resin LR 73.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
Micropol Microlink XL28 Crosslinkable Polyethylene Provides a finished molding of improved properties with the use of conventional rotational molding equipment. Properties include enhanced toughness (particularly low temp impact), ESCR, chemical, a.. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xylex HX7409HP PC+POLYESTER (Europe-Africa-Middle East) Low flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change (MoC), biocompatible (ISO 10993 or USP Class VI).. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL NH4030B PPE+HIPS (Asia Pacific) NH4030B is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nory.. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL NH4030B PPE+HIPS (Europe-Africa-Middle East) NH4030B is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nory.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
ExxonMobil HDPE AP60-007 High Density Polyethylene Resin Product Description: AP60-007 is a medium molecular weight distribution high density polyethylene homopolymer. It possesses excellent processing uniformity and produces bottles with excellent appear.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
ExxonMobil Optema® TC-110 Blown Ethylene Methyl Acrylate Product Description: Optema TC 110 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown film applications. It produces a soft, elast.. |
|||
Vicat Softening Point | 127 °C @Load 1.00 kg |
261 °F @Load 2.20 lb |
ASTM D1525 |
Diamond Polymers ABS TS15v04 Injection Molding Grade, ABS/PC Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
Dow UNIVAL™ DMDA-6147 NT 7 High Density Polyethylene Resin (HDPE) Good extrudability/processability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6147 NT 7 is a polymer with broad molecular weight distribution and high molecular weight. This produ.. |
|||
Vicat Softening Point | 127 °C | 260 °F | ASTM D1525 |
ExxonMobil Paxon™ AD60-007 Blow Molding Resin Product Description: AD60-007 is a medium molecular weight distribution high-density polyethylene homopolymer. It possesses excellent processing uniformity and produces bottles with excellent appear.. |
|||
Vicat Softening Point | 127 °C | 261 °F | 10 N; ASTM D1525 |
Braskem RP 141 Injection Molding Polypropylene Description: RP 141 is a high melt flow rate random copolymer designed for injection molding. This product offers outstanding transparency, very good stiffness/impact strength balance and excellent .. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
NOVA Chemicals Sclair® D916-39 HDPE Extrusion Resin
(discontinued **) Features: Excellent processability, excellent stretchability, high stiffness, superior strength, gel free, excellent UV resistance.Applications: Industrial woven bags, tarpaulins.Data provided by th.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
Braskem BU 004 HDPE Blow Molding Polyethylene Applications: Bottles for food products, lubricating and cooking oil; toys; bottler for surface-active agents; sheets. Information provided by Braskem |