| Category | Polymer , Thermoplastic , Polycarbonate (PC) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Lexan® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics Lexan® FL930 PC.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.29 g/cc | 1.29 g/cc | foam molded; ASTM D792 |
| 1.43 g/cc | 1.43 g/cc | ASTM D792 | |
| Water Absorption | 0.12 % <br>@Time 86400 sec |
0.12 % <br>@Time 24.0 hour |
ASTM D570 |
| Moisture Absorption at Equilibrium | 0.26 % | 0.26 % | ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm <br>@Thickness 6.40 mm |
0.0020 - 0.0040 in/in <br>@Thickness 0.252 in |
SABIC Method |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 72.0 MPa <br>@Thickness 6.35 mm |
10400 psi <br>@Thickness 0.250 in |
ASTM D638 |
| Elongation at Break | 3.0 % <br>@Thickness 6.35 mm |
3.0 % <br>@Thickness 0.250 in |
ASTM D638 |
| Tensile Modulus | 6.92 GPa <br>@Thickness 6.40 mm |
1000 ksi <br>@Thickness 0.252 in |
ASTM D638 |
| Flexural Yield Strength | 127 MPa | 18400 psi | 6.4 mm; ASTM D790 |
| Flexural Modulus | 6.89 GPa | 999 ksi | 6.4 mm; ASTM D790 |
| Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
| Dart Drop, Total Energy | 40.0 J | 29.5 ft-lb | SABIC Method |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 21.6 µm/m-°C <br>@Temperature -40.0 - 95.0 °C |
12.0 µin/in-°F <br>@Temperature -40.0 - 203 °F |
ASTM E 831 |
| Specific Heat Capacity | 1.04 J/g-°C | 0.249 BTU/lb-°F | ASTM C351 |
| Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | ASTM C177 |
| Deflection Temperature at 0.46 MPa (66 psi) | 143 °C <br>@Thickness 6.40 mm |
289 °F <br>@Thickness 0.252 in |
unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 138 °C <br>@Thickness 6.40 mm |
280 °F <br>@Thickness 0.252 in |
unannealed; ASTM D648 |
| UL RTI, Electrical | 110 °C | 230 °F | UL 746B |
| UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
| UL RTI, Mechanical without Impact | 110 °C | 230 °F | UL 746B |
| Flammability, UL94 | V-0 <br>@Thickness 5.99 mm |
V-0 <br>@Thickness 0.236 in |
UL 94 |
| 5VA <br>@Thickness 5.99 mm |
5VA <br>@Thickness 0.236 in |
UL 94 | |
| Oxygen Index | 40.4 % | 40.4 % | ASTM D2863 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 2.40e+17 ohm-cm | 2.40e+17 ohm-cm | ASTM D257 |
| Surface Resistance | >= 1.10e+17 ohm | >= 1.10e+17 ohm | ASTM D257 |
| Dielectric Constant | 2.61 <br>@Frequency 1.00e+6 Hz |
2.61 <br>@Frequency 1.00e+6 Hz |
ASTM D150 |
| 2.7 <br>@Frequency 100 Hz |
2.7 <br>@Frequency 100 Hz |
ASTM D150 | |
| Dissipation Factor | 0.0034 <br>@Frequency 100 Hz |
0.0034 <br>@Frequency 100 Hz |
ASTM D150 |
| 0.0075 <br>@Frequency 1.00e+6 Hz |
0.0075 <br>@Frequency 1.00e+6 Hz |
ASTM D150 | |
| Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | Tungsten; ASTM D495 |
| Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | UL 746A |
| High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min | UL 746A |
| Descriptive Properties | Value | Comments |
|---|---|---|
| FOAM - ELECTRICAL 6.4 mm Wt Reduction | 20% | |
| FOAM - Flame Class Minimum Density | 0.9g/cm^3 | |
| FOAM - IMPACT 6.4 mm Wt Reduction | 10% | |
| FOAM - MECHANICAL 6.4 mm Wt Reduction | 10% | |
| FOAM - PHYSICAL 6.4mm Wt Reduction | 10% | |
| FOAM - THERMAL 6.4mm Wt Reduction | 10% |