Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ASTM D638 |
NYCOA 2062 Copolymer Nylon 6/66 FDA approved extrusion grade for film.Information provided by NYCOA, Inc. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® 505RU PC (Asia Pacific) Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro.. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® DMX9254 PC (Europe-Africa-Middle East) Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl.. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer High viscosity Proprietary Polycarbonate Ester, OSU 55/55 compliant, low smoke, flame retardant resin |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer (Asia Pacific) High visocisty PC Copolymer, OSU 55/55 compliant, low smoke, flame retardant resin |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer (Europe-Africa-Middle East) High viscosity PC Copolymer, OSU 55/55 compliant, low smoke, flame retardant resin |
|||
Tensile Strength, Yield | 71.5 MPa @Temperature 23.0 °C |
10400 psi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 127UV BK701 Acetal Homopolymer
(Unverified Data**) Delrin® 127UV BK701 is a high viscosity, UV stabilized acetal homopolymer. It has excellent impact strength, UV resistance and thermal stability. It is well suited for automotive interior applicati.. |
|||
Tensile Strength, Yield | 72.0 MPa @Temperature 23.0 °C |
10400 psi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 150 NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has excellent thermal stability, low die deposit, and enhanced crystallization for low porosity.Information pr.. |
|||
Tensile Strength, Yield | 72.0 MPa @Temperature 23.0 °C |
10400 psi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 988PA NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 988PA NC010 is a low viscosity acetal homopolymer for injection molding with low screw deposit. It is especially formulated for gear applications requiring high precision and dimensional st.. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ASTM D638 |
Plaskolite Optix® PL-30 Acrylic Resin
(discontinued **) Injection molding and extrusion grade pellets. Highest molecular weight and heat resistance of Optix® line with exceptional mold release.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Tensile Strength, Yield | 71.6 MPa @Thickness 3.20 mm |
10400 psi @Thickness 0.126 in |
ASTM D638 |
LG Chemical LUMILOY GN1306F Injection Molding FR Heat Resistant mPPO Uses include electric/electronic parts. |
|||
Tensile Strength, Yield | 72.0 MPa @Temperature 22.0 °C |
10400 psi @Temperature 71.6 °F |
25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 0180 Unsaturated Polyester UP SMC 0180 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRILOY UX98388 PPA LNP LUBRILOY* UX98388 is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp OK006 PPS - Linear LNP* Thermocomp* OK006 is based on a Linear Polyphenylene Sulfide (PPS) containing Talc.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl LS175 PPE+HIPS Noryl* LS175 modified polyphenylene ether resin is an unfilled grade suitable for both extrusion and injection molding conversion routes. It uses non-chlorinated, non-brominated FR additives to del.. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl LS175 PPE+HIPS (Europe-Africa-Middle East) Noryl* LS175 modified polyphenylene ether resin is an unfilled grade suitable for both extrusion and injection molding conversion routes. It uses non-chlorinated, non-brominated FR additives to del.. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL N1150 PPE+PS (Asia Pacific) Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add.. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP 9X10401H ABS LNP* THERMOCOMP* 9X10401H is a compound based on Polyphenylsulfone containing proprietary filler(s). Added feature of this grade is: X-Ray Opaque. |
|||
Tensile Strength, Yield | 72.0 MPa @Thickness 6.35 mm |
10400 psi @Thickness 0.250 in |
ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM3020 PPE+PS LNP* Thermocomp* Noryl_FM3020 compound is GR/MR 30%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL LTA6020 PPE+PS (Europe-Africa-Middle East) |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ASTM D638 |
Tipco Tipcofil® AM 300 - 15% Mineral Reinforced Nylon-6 Compound, with High Heat Stability 15% Mineral Reinforced Nylon-6 CompoundApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO 527-1/-2 |
Covestro Apec® 1795 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=173°CPreprocessingMax. Water content |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO 527-1/-2 |
Covestro Apec® 1803 Polycarbonate UV-stabilizedsoftening temperature (VST/B 120)=184 °CPreprocessingMax. Water content |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO 527-1/-2 |
Covestro Apec® DP1-9354 Polycarbonate, Flame Retardant Grade Developmental productflame retardant: V-0/1,5mm (UL 94)V-0/3,0mm (UL 94)5VA/3mm (UL 94)softening temperature (VST/B 120)=185 °Conly opaque colors availablePreprocessingMax. Water content |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 100PE BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100PE BK602 (formerly DE20573) is a high viscosity acetal homopolymer an enhanced version of Delrin 100P with very low VOC emissions... |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 111DP NC010 Acetal (POM)
(Unverified Data**) Nucleated High Viscosity Acetal Homopolymer Delrin 111DP is a new high viscosity acetal homopolymer with enhanced crystallization and excellent creep and fatigue resistance. It has improved thermal .. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 150 NC010 Acetal (POM)
(Unverified Data**) Nucleated High Viscosity Acetal Homopolymer Developed for Extrusion Delrin 150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has excellent thermal stability low die deposi.. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® II150E BK602 Acetal (POM) Nucleated High Viscosity Acetal Homopolymer Developed for ExtrusionInformation provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 71.7 MPa | 10400 psi | ASTM D638 |
Entec Hyril® GP355AS Styrene Acrylonitrile Available in North America Features: Copolymer Automotive Specifications: DELPHI M-9565-9 Color: Blue-TransparentForm: PelletsProcessing Method: ExtrusionInformation provided by Entec |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP GX94043L PSU (Europe-Africa-Middle East) LNP* THERMOCOMP* GX94043L is a compound based on Polysulfone resin containing Mineral. |