Material Notes:
Grade for calanderingno yellowing under the action of UV lightgood low-temperature flexibilityhigh rebound resilienceimproved microbial resistanceImproved hydrolysis resistanceApplicationTextile coatingPreprocessingMax. Water content
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
3s; ISO 868
Tensile Strength at Break 26.0 MPa
3770 psi
ISO 527-1/-2
Tensile Strength, Yield 26.0 MPa
3770 psi
parallel; ISO 527-3
6.30 MPa

@Strain 100 %
914 psi

@Strain 100 %
ISO 527-1/-2
9.50 MPa

@Strain 300 %
1380 psi

@Strain 300 %
ISO 527-1/-2
Elongation at Break >= 300 %
>= 300 %
ISO 527-1/-2
Abrasion 30
30
mm³; ISO 4649
Compression Set 12 %

@Temperature 23.0 °C
12 %

@Temperature 73.4 °F
ISO 815
43 %

@Temperature 70.0 °C
43 %

@Temperature 158 °F
ISO 815