Material Notes:
Data provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Density 0.925 g/cc
0.0334 lb/in³
ASTM D792
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
ASTM D955
Melt Flow 8.0 g/10 min
8.0 g/10 min
Mechanical Properties Metric English Comments
Hardness, Shore D 45
45
ASTM D2240
Tensile Strength, Yield 16.5 MPa
2400 psi
ASTM D638
Flexural Modulus 0.517 GPa
75.0 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256