Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 72.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 72.0 MPa
10400 psi
ASTM D638
Plaskolite Optix® PL-25 Acrylic Resin
Extrusion grade pellets. Highest molecular weight and heat resistance of Optix® line.Data provided by the manufacturer, Plaskolite, Inc.
Tensile Strength, Yield 72.0 MPa
10400 psi
ASTM D638
Nylene® 733 Nylon 6
Dry as molded. Injection molding grade. Nylene 733 is a high impact modified nylon suitable for both molding and extrusion. Parts molded from 733 have excellent impact strength right out of the mol..
Tensile Strength, Yield 72.0 MPa
10400 psi
5 mm/min; ISO 527
SABIC Innovative Plastics Lexan® 505RU PC (Europe-Africa-Middle East)
Lexan* 505RU is a 10% glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEE..
Tensile Strength, Yield 72.0 MPa
10400 psi
Type I, 50 mm/min; ASTM D 638
SABIC Innovative Plastics Lexan® DMX9254 PC (Asia Pacific)
Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl..
Tensile Strength, Yield 72.0 MPa
10400 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP DFL22 PC (Asia Pacific)
LNP* Lubricomp* DFL22 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Tensile Strength, Yield 72.0 MPa

@Temperature 23.0 °C
10400 psi

@Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Delrin® 150 NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has excellent thermal stability, low die deposit, and enhanced crystallization for low porosity.Information pr..
Tensile Strength, Yield 72.0 MPa

@Thickness 6.35 mm
10400 psi

@Thickness 0.250 in
ASTM D638
SABIC Innovative Plastics Lexan® FL933 PC
Various weight reductions at 0.250"" wall. 30% GR. Superior flexural strength and modulus; good tensile strength. UV-stabilized.
Tensile Strength, Yield 72.0 MPa
10400 psi
ASTM D638
Plaskolite Optix® PL-30 Acrylic Resin  (discontinued **)
Injection molding and extrusion grade pellets. Highest molecular weight and heat resistance of Optix® line with exceptional mold release.Data provided by the manufacturer, Plaskolite, Inc.
Tensile Strength, Yield 72.0 MPa

@Temperature 22.0 °C
10400 psi

@Temperature 71.6 °F
25mm flat samples, compression moulded; ISO 527-4
Menzolit Menzolit® SMC 0180 Unsaturated Polyester UP
SMC 0180 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t..
Tensile Strength, Yield 72.0 MPa
10400 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1510A PC
LNP* Lubricomp* Lexan_LF1510A compound is a 10% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances.
Tensile Strength, Yield 72.0 MPa
10400 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1510A PC (Asia Pacific)
10% glass reinforced/15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances.
Tensile Strength, Yield 72.0 MPa
10400 psi
2 in/min; ASTM Test
Styrolution Luran® 358 N SAN
Luran 358 N is an easy-flowing injection molding SAN grade.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
Tensile Strength, Yield 72.0 MPa
10400 psi
ISO 527
Styrolution Luran® HD 20 SAN
Luran HD 20 is an easy-flow grade of SAN especially designed for the medical market. It is suitable for moldings with very thin walls and / or adverse flow length to wall ratio. It features very goo..
Tensile Strength, Yield 72.0 MPa
10400 psi
Type I, 5 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp OK006 PPS - Linear
LNP* Thermocomp* OK006 is based on a Linear Polyphenylene Sulfide (PPS) containing Talc.This data was supplied by SABIC-IP for the Americas region.
Tensile Strength, Yield 72.0 MPa
10400 psi
50 mm/min; ISO 527
SABIC Innovative Plastics Noryl LS175 PPE+HIPS
Noryl* LS175 modified polyphenylene ether resin is an unfilled grade suitable for both extrusion and injection molding conversion routes. It uses non-chlorinated, non-brominated FR additives to del..
Tensile Strength, Yield 72.0 MPa
10400 psi
50 mm/min; ISO 527
SABIC Innovative Plastics NORYL N1150 PPE+PS (Asia Pacific)
Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add..
Tensile Strength, Yield 72.0 MPa
10400 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-LOY PF303 PA 6
LNP* STAT-LOY* PF303 is a Nylon 6 base resin containing 15% Glass Fiber. Added features of this grade includes: Antistat.
Tensile Strength, Yield 72.0 MPa
10400 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP 9X10401H ABS
LNP* THERMOCOMP* 9X10401H is a compound based on Polyphenylsulfone containing proprietary filler(s). Added feature of this grade is: X-Ray Opaque.
Tensile Strength, Yield 72.0 MPa

@Thickness 6.35 mm
10400 psi

@Thickness 0.250 in
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM3020 PPE+PS
LNP* Thermocomp* Noryl_FM3020 compound is GR/MR 30%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness.
Tensile Strength, Yield 72.0 MPa

@Thickness 4.00 mm
10400 psi

@Thickness 0.157 in
50mm/min, injection molded, unannealed; ISO 527-2
Styron EMERGEâ„¢ 5302 Acrylonitrile Butadiene Styrene (ABS)
EMERGEâ„¢ ABS 5302 is a black, 20% glass-filled ABS which is suitable for use in a wide variety of internal structural component applications in the information technology market. Applications: ..
Tensile Strength, Yield 72.0 MPa
10400 psi
50 mm/min; ISO 527
SABIC Innovative Plastics NORYL N1150 PPE+PS (Europe-Africa-Middle East)
Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add..
Tensile Strength, Yield 72.0 MPa
10400 psi
ISO 527-1/-2
DuPont Performance Polymers Delrin® 111DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated High Viscosity Acetal Homopolymer Delrin 111DP is a new high viscosity acetal homopolymer with enhanced crystallization and excellent creep and fatigue resistance. It has improved thermal ..
Tensile Strength, Yield 72.0 MPa
10400 psi
ISO 527-1/-2
DuPont Performance Polymers Delrin® 150 NC010 Acetal (POM)  (Unverified Data**)
Nucleated High Viscosity Acetal Homopolymer Developed for Extrusion Delrin 150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has excellent thermal stability low die deposi..
Tensile Strength, Yield 72.0 MPa
10400 psi
ISO 527-1/-2
DuPont Performance Polymers Delrin® 527UVE NC010 Acetal (POM)  (Unverified Data**)
UV Stabilized Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 527UVE NC010 (formerly DE20556) is a medium viscosity acetal homopolymer with UV stabilizers with very low VOC emissi..
Tensile Strength, Yield 72.0 MPa
10400 psi
ASTM D638
Evonik CYRO Acrylite® DQ 501 Compound Molding and Extrusion
ACRYLITE® SuPure™ acrylic polymer is an exceptional pure polymer designed for applications that demand maximum cleanliness. Our proprietary purification process starts at CYRO’s manufacturing pla..
Tensile Strength, Yield 72.0 MPa
10400 psi
ISO 527-1/-2
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and ..
Tensile Strength, Yield 72.0 MPa
10400 psi
ISO 527-1/-2
DuPont Performance Polymers Delrin® FG150 NC010 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer Developed for Food Contact ApplicationsDelrin FG150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has low die deposit and low porosity. I..
Tensile Strength, Yield 72.0 MPa
10400 psi
23°C, 50% RH; ASTM D638
Asahi Kasei Xyron® SZ800 Modified Polyphenylene Ether
High-Heat ResistantInformation provided by Asahi Kasei
Tensile Strength, Yield 72.0 MPa

@Temperature 23.0 °C
10400 psi

@Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Delrin® FG150 NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® FG150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has low die deposit and low porosity. It has been developed for consideration in applications and parts for th..
Tensile Strength, Yield 72.0 MPa
10400 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP GX94043L PSU (Europe-Africa-Middle East)
LNP* THERMOCOMP* GX94043L is a compound based on Polysulfone resin containing Mineral.
Copyright © lookpolymers.com All Rights Reserved