Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Lexan® 2014R PC (Europe-Africa-Middle East) LEXAN 2014R is a medium viscosity flame retardant grade, This material contains a release agent to ensure easy processing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region... |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Lexan® 503 PC 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Lexan® 503 PC (Asia Pacific) 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Lexan® 503R PC 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. Internal mold release. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Lexan® 503R PC (Asia Pacific) 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. Internal mold release. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Lexan® 503R PC (Europe-Africa-Middle East) LEXAN 503R is a medium viscosity, 10% glass reinforced, UV-stabilized, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance and exce.. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Lexan® FL920 PC Various weight reductions at .250"" (6.35 mm) wall, 20% GR. Excellent flex mod, high tensile strength/heat resistance. V-0/5V at .250"" (6.35mm). |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Lexan® ML7682 PC Copolymer (Asia Pacific) Lexan ML7682 resin is a flame retardant polycarbonate blend featuring high flow, good processability, good impact, good heat resistance, and UV stability. It is of non-chlorine and non-bromine flame.. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Lexan® FL930 PC Various weight reductions at 0.250"" (6.35 mm) wall, 30% GR. Superior flex strength/modulus, good tensile strength. V-0/5VA at 0.250"" (6.35 mm). |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Lexan® FL930 PC (Asia Pacific) Various weight reductions at 0.250"" (6.35 mm) wall, 30% GR. Superior flex strength/modulus, good tensile strength. V-0/5VA at 0.250"" (6.35 mm). |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | Minimum thickness 0.040 inches. |
LyondellBasell Pro-fax 6523 Polypropylene Homopolymer, General Purpose Key Features: general purpose polypropylene homopolymer resin, stiff, high resistance to solvents, FDA acceptableApplications: automotive, hospital and institutional ware, housewares, general moldin.. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL746B |
Idemitsu Kosan Xarec® EA 543 SPS, 40% Glass Filled |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL746B |
Idemitsu Kosan Xarec® WA 212 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled, Impact Modified. Used in Automotive and Industrial applications. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | |
LG Chemical LUPOY GN1006FT PC, Halogen Free, Flame Retardant Description: Injection Molding, PC, Halogen Free Flame Retardant, Good FlowApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 110 °C @Thickness 1.60 mm |
230 °F @Thickness 0.0630 in |
|
LyondellBasell Higlass SB224-3 Polypropylene Copolymer, 30% Glass Fiber Key Features: conventional melt flow, medium high modulus, chemically coupled, glass fiber-reinforced polypropylene copolymer, high impact strength, high stiffness, good processabilityApplications: .. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Valox® 553 PBT+PC 30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Valox® 553U PBT+PC 30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Valox® 815 PBT 15% GR PBT+ PET, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Valox® 865 PBT+PET 30% GR PBTP, UL94 V-0 rated. Non-blooming flame retardant. Improved surface appearance. Same application areas as for VALOX 855. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Valox® 865 PBT+PET (Asia Pacific) 30% GR PBTP, UL94 V-0 rated. Non-blooming flame retardant. Improved surface appearance. Same application areas as for VALOX 855. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746 |
Styron EMERGEâ„¢ 4610-10 Polycarbonate EMERGEâ„¢ PC 4610-10 advanced resin is formulated to deliver both outstanding clarity and enhanced ignition resistance while maintaining excellent physical properties and processability. Applica.. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL GTX GTX918W PPE+PA (Europe-Africa-Middle East) NORYL GTX918W is an unfilled global grade, which offers an excellent combination of processability and heat resistance. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Valox® 815 PBT (Asia Pacific) 15% GR PBTP, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746 |
Styron EMERGEâ„¢ 4701-13 Polycarbonate EMERGEâ„¢ PC 4701-13 advanced resin is formulated with 10% glass fiber and a proprietary flame retardant package. It provides good ignition resistance, rigidity, dimension stability and heat res.. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 (Europe-Africa-Middle East) LNP VERTON* RV00AES is a compound based on PA 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics LNP VERTON RV00AESC PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AESC is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding, Heat Stabilized. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | |
Covestro Makrolon® 6485 Polycarbonate, Injection Grade Medium viscosity, flame retardant injection molding grade with easy mold release, not available in transparent colors.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was .. |
|||
UL RTI, Mechanical with Impact | 110 °C @Thickness 1.50 mm |
230 °F @Thickness 0.0591 in |
746B |
BASF Ultramid® KR 4357 G6 30% Glass Filled PA6/6T (Dry) Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan.. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics LNP VERTON RV00ASXS PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00ASXS is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Heat Stabilized |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Valox® VX5530 PBT (Europe-Africa-Middle East) VALOX VX5530 is a flame retarded, 15% glass fibre reinforced, 10% mineral filled PBT+PC blend with excellent low warpage characteristics.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |