A. Schulman ComAlloy E-16903B Nylon 6/6, Electrically Conductive - Stainless Steel Fiber Filled

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Conductive
Manufacturer A. Schulman ComAlloy
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy E-16903B Nylon 6/6, Electrically Conductive - Stainless Steel Fiber Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 117
117
ASTM D785
Tensile Strength, Ultimate 97.0 MPa
14100 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Yield Strength 165 MPa
23900 psi
ASTM D790
Flexural Modulus 8.00 GPa
1160 ksi
ASTM D790
Izod Impact, Unnotched 3.20 J/cm
5.99 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 255 - 275 °C
491 - 527 °F
Deflection Temperature at 0.46 MPa (66 psi) 252 °C
486 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 183 °C
361 °F
ASTM D648
Electrical Properties Metric English Comments
Electrical Resistivity 1.00 - 10.0 ohm-cm
1.00 - 10.0 ohm-cm
Surface Resistance 10 - 100 ohm
10 - 100 ohm