Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Wire & Cable W1820L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
SABIC Innovative Plastics Lexan® LGK3020 PC (Asia Pacific) Glass reinforced. Flame retardant. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible C90A0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible R363MB White 1876 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 80-0837-1 Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Specific Gravity | 1.43 - 1.45 g/cc | 1.43 - 1.45 g/cc | ASTM D792 |
Loxim 130 01V0 Polycarbonate, 30% Glass Filled, Flame Retardant Information provided by Loxim Industries |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
LTL Color Compounds ColorFast® PCGF130 Polycarbonate, 30% Glass-Filled 30% glass-filled grade polycarbonateAll information provided by LTL Color Compounders, Inc. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | |
Momentive Performance Materials Siloprenâ„¢ FFSL 7286/40 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D 792 |
SABIC Innovative Plastics Ultem 2212 PEI 20% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON DEL36 PC LNP* STAT-KON* DEL36 is a compound based on Polycarbonate resin containing 30% Carbon Fiber, 15% PTFE. Added features include: Electrically Conductive, Wear Resistant. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | |
Shinil Chemical SHINCON PEEK-CF LCD Rack LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since b.. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | |
Shinil Chemical SHINFLAME PBT Flame Retardant Polymer Connector SHINFLAME is a flame retardant (FR) compound which exhibits inherent flame retardant properties during fire. Shinil uses its patented dispersion blending technology with variety of polymers to prod.. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP DF006HL PC LNP THERMOCOMP* DF006HL is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Low Extractible, Healthcare. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
Techmer ES Plaslube® J-1/20/TF/20 BK PA66 |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
Teknor Apex Sinvicomp SRP 5602 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: Good ProcessabilityUses: Conduit; Piping; Profiles Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Canyon 10277U/4 Concentrate Based In LLDPE DescriptionPOLYBATCH® 10277U/4 is a canyon color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provided color and UV stabil.. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Blue 4021 Concentrate Based in Polyethylene DescriptionPOLYBATCH® 4021 is a blue color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 4021 is typi.. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Blue 4021 Concentrate Based in Polyethylene DescriptionPOLYBATCH® 4021 is a blue color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 4021 is typi.. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
A. Schulman SCHULAMID® 66 GB40 40% Glass Bead Reinforced Nylon 66 Information provided by A. Schulman. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
Colorite Polymers 93-635A General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Specific Gravity | 1.43 - 1.47 g/cc | 1.43 - 1.47 g/cc | ASTM D-792 |
Axiall 971 Wire & Cable Flexible PVC Matte-finish, CL2 jacket compound rated for 90°C applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | |
Aremco Corr-Paint™ CP4070-S High Temperature Protective Coating, Silicone-Polyester |
|||
Specific Gravity | 1.43 - 1.47 g/cc | 1.43 - 1.47 g/cc | ASTM D-792 |
Axiall 12880 Coax & Telecom Flexible PVC VW-1 coax cable jacket. RG 6.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | Absolute Drying; ASTM-D792 |
Toyobo GLAMIDE® T-779 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D 792 |
SABIC Innovative Plastics Valox® VC108 PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |