Thermal Properties Metric English Comments
Specific Heat Capacity 1.04 J/g-°C
0.249 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® 3414R PC
40% GR, provides improved mechanical properties and UL94V-1 rated at 0.058"". Internal mold release added.
Specific Heat Capacity 1.04 J/g-°C
0.249 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® 3414R PC (Asia Pacific)
40% GR, provides improved mechanical properties and UL94V-1 rated at 0.058"". Internal mold release added.
Specific Heat Capacity 1.04 J/g-°C
0.249 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® FL930 PC
Various weight reductions at 0.250"" (6.35 mm) wall, 30% GR. Superior flex strength/modulus, good tensile strength. V-0/5VA at 0.250"" (6.35 mm).
Specific Heat Capacity 1.04 J/g-°C
0.249 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® FL930 PC (Asia Pacific)
Various weight reductions at 0.250"" (6.35 mm) wall, 30% GR. Superior flex strength/modulus, good tensile strength. V-0/5VA at 0.250"" (6.35 mm).
Specific Heat Capacity 1.04 J/g-°C
0.249 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® FL933 PC
Various weight reductions at 0.250"" wall. 30% GR. Superior flexural strength and modulus; good tensile strength. UV-stabilized.
Specific Heat Capacity 1.04 J/g-°C
0.249 BTU/lb-°F
Specialty Coating Systems Parylene HT® Poly (P-Xylylene) Coating
Parylene HT is a polymer of para-xylylene with the alpha hydrogen atoms of the N dimer replaced with fluorine. This variant of Parylene is useful in high temperature applications (short term up to 4..
Specific Heat Capacity 1.04 J/g-°C
0.249 BTU/lb-°F
Ensinger TECASINT 1011 Polyimide (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
Specific Heat Capacity 1.04 J/g-°C
0.249 BTU/lb-°F
Ensinger TECASINT 1101 Polyimide (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
Specific Heat Capacity 1.04 J/g-°C
0.249 BTU/lb-°F
Ensinger TECASINT 4011 Polyimide, Yellow (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
Specific Heat Capacity 1.04 J/g-°C
0.249 BTU/lb-°F
Product Property; E1461-01
Arlon Thermabond® 48991A010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate
Description: Generation IIa Thermabond® NP electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style ..
Copyright © lookpolymers.com All Rights Reserved