Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | DIN 52612 |
Polycasa PS QUINN PS sheets have good optical properties and a brilliant surface. The QUINN PS range contains sheets that are easy to fabricate, to vacuum form, and show a high light transmission (min 88% wavel.. |
|||
Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | DIN 52612 |
Ineos Nova S-2200 Medium Impact Compact Polystyrene
(discontinued **) Medium impact easy flowing polystyrene, designed for injection molding applications with short cycle times and for complicated technical parts. The product has a high stiffness and an excellent the.. |
|||
Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | DIN 52612 |
Ineos Nova S-3401 Medium Impact Compact Polystyrene
(discontinued **) Impact polystyrene with good flow characteristics and a high elongation. Generally used for applications where a tough material is required. The material is provided with external lubricate to imp.. |
|||
Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | DIN 52612 |
Ineos Nova S-3500MG Compact Polystyrene Microgranulates
(discontinued **) Very easy flowing medium impact polystyrene Microgranulates, having a diameter of 0.8 - 1.0 mm and a very large specific surface areas. This grade is especially designed for use in compounding and .. |
|||
Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | DIN 52612 |
Ineos Nova S-4600 High Impact Compact Polystyrene
(discontinued **) High impact polystyrene with excellent flow characteristics, a very high toughness and a high elongation. Main application are injection molding of technical parts and housings. For injection mold.. |
|||
Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | DIN 52612 |
Ineos Nova S-6600MG Compact Polystyrene Microgranulates
(discontinued **) High impact polystyrene Microgranulates, having a diameter of 0.8 - 1.0 mm especially useful for compounding and extrusion applications. Due to the higher viscosity intensive mixing with thermoplas.. |
|||
Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® FL930 PC Various weight reductions at 0.250"" (6.35 mm) wall, 30% GR. Superior flex strength/modulus, good tensile strength. V-0/5VA at 0.250"" (6.35 mm). |
|||
Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® FL930 PC (Asia Pacific) Various weight reductions at 0.250"" (6.35 mm) wall, 30% GR. Superior flex strength/modulus, good tensile strength. V-0/5VA at 0.250"" (6.35 mm). |
|||
Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® FL933 PC Various weight reductions at 0.250"" wall. 30% GR. Superior flexural strength and modulus; good tensile strength. UV-stabilized. |
|||
Thermal Conductivity | 0.160 - 0.432 W/m-K | 1.11 - 3.00 BTU-in/hr-ft²-°F | Average value: 0.342 W/m-K Grade Count:3 |
Overview of materials for Nylon 12, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | Through Thickness |
GrafTech P1 PET Film Optional coating for eGRAF® SPREADERSHIELD™ graphite products. Structure: Plastic 0.0127mm - Adhesive 0.0127mm - Graphite |
|||
Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | Through Thickness |
GrafTech P2 PET Film Optional coating for eGRAF® SPREADERSHIELD™ graphite products. Structure: Plastic 0.0014mm - Adhesive 0.008mm - Graphite |
|||
Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | ASTM C177 |
KYDEX® 100 Acrylic/PVC Thermoplastic Sheet High impact fire rated sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones. Hidden parts for equipment such as vending machines.. |
|||
Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Valox® 325 PBT (Europe-Africa-Middle East) VALOX 325 is a general purpose, unreinforced PBT injection moulding resin. Applications: sprinklers and nozzles, pumps, doorhandles, tank covers, pens and pencils. |
|||
Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Valox® FXV310SK PBT (Europe-Africa-Middle East) LIMITED USE, No New Customers / Applications as of Jan. 2010: VALOX FXV310SK is an unreinforced PBT injection moulding resin with high flow characteristics and containing a metal sparkle Visual FX. .. |
|||
Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | DIN 52612-1 |
Styrolution PS 116 N/L GPPS Styrolution PS 116N/L is a general purpose polystyrene grade with excellent flow properties and improved heat resistance.Excellent flow propertiesHigh heat resistanceInformation provided by Styrolut.. |
|||
Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | DIN 52612-1 |
Styrolution PS 124 N/L GPPS Styrolution PS 124N/L is a general purpose polystyrene grade with a good flow characteristic and an improved heat resistance.Excellent flow propertiesHigh heat resistanceUL 94 HB (Antwerp only)Infor.. |
|||
Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | DIN 52612-1 |
Styrolution PS 153F GPPS Styrolution PS 153F is general purpose polystyrene with high heat resistance and good flow properties. Styrolution PS 153F is free of internal lubricants, e.g. zinc stearate.Free of internal lubrica.. |
|||
Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | DIN 52612-1 |
Styrolution PS 416N HIPS Styrolution PS 416N is medium impact polystyrene with very good flow properties. It has a high rigidity whilst displaying a very good surface gloss.Very good flow propertiesHigh rigidityVery good su.. |
|||
Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | DIN 52612-1 |
Styrolution PS 542N HIPS Styrolution PS 542N is an impact polystyrene with high heat resistance.Information provided by Styrolution |
|||
Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | |
Goodfellow Topas® Cyclo-olefin copolymer Information provided by Goodfellow. |
|||
Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | Melt |
Covestro Bayblend® T88 GF-20* Polycarbonate + SAN Glass Filled Impact Grade Developmental productInjection molding grade20 % GFoptimized heat ageing- and UV-stabilityvery good flowtensile modulus = 7500 MPaVicat/B 120 = 130 °CPreprocessingMax. Water content |
|||
Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | of melt |
DuPont Performance Polymers Zytel® FG101L NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66 with Developed for Food Contact ApplicationsZytel FG101L NC010 is a lubricated polyamide 66 resin for injection molding. It has been developed for consideration into applic.. |
|||
Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | of melt |
DuPont Performance Polymers Zytel® FG408L NC010 Nylon 66
(Unverified Data**) Unreinforced Toughened Polyamide 66 with Developed for Food Contact Applications Zytel FG408L NC010 is a general purpose lubricated impact modified polyamide 66 resin with superior toughness for inj.. |
|||
Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | of melt |
DuPont Performance Polymers Zytel® FG42L NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers |
|||
Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | of melt |
DuPont Performance Polymers Zytel® FN727 NC010A Nylon 6
(Unverified Data**) Toughened Polyamide 6Information provided by DuPont Performance Polymers |
|||
Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | of melt |
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | DIN 52612 |
Ineos Nova S-4122 Medium Impact Compact Polystyrene
(discontinued **) Low friction, medium impact polystyrene which combines excellent flow characteristics with a good dimensional stability under heat and a high stiffness. This grade is designed for injection moldin.. |
|||
Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | |
Pyrotek ISOCAST Insulating Refractory Castable Pyrotek's Isocast is a refractory castable based on phosphate bonded calcium silicate material. Isocast exhibits excellent thermal insulation characteristics and very good behavior with respec.. |
|||
Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | of melt |
DuPont Performance Polymers Zytel® 101F NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101F NC010 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont .. |