SABIC Innovative Plastics LNP LUBRICOMP QFP36 PA6.10 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 610
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP QFP36 PA6.10 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* QFP36 is a compound based on PA6.10 resin containg Glass Fiber, PTFE, Silicone. Added features include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 118 MPa
17100 psi
5 mm/min; ISO 527
Elongation at Yield 3.0 %
3.0 %
5 mm/min; ISO 527
Tensile Modulus 8.10 GPa
1170 ksi
1 mm/min; ISO 527
Flexural Yield Strength 165 MPa
23900 psi
2 mm/min; ISO 178
Flexural Modulus 6.20 GPa
899 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²
5.71 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 23.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
12.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 100 µm/m-°C

@Temperature 23.0 - 60.0 °C
55.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 198 °C
388 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 HB

@Thickness 0.750 mm
HB

@Thickness 0.0295 in
UL 94