Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Transverse to Flow = 100 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-2
Celanese Celanex® 2008 PBT  (Unverified Data**)
Celanex 2008 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in melt blown applications.Ultrahigh melt flowInfor..
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-2
Celanese Celanex® 3300-2 PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3300-2 is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outsta..
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-2
Celanese Celanex® 4202 PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 4202 is a 15% glass reinforced, impact modified polybutylene terephthalate with excellent surface appearance.15% glass-fiber, improved impactInformation provided by Celanese
CTE, linear, Transverse to Flow 100 µm/m-°C

@Temperature 23.0 - 60.0 °C
55.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics GELOY CR7020 ASA (Europe-Africa-Middle East)
GELOY CR7020 is a profile extrusion and co-extrusion grade, blend of ASA/SAN. In co-extrusion it can be used over CYCOLAC, PVC or other compatible polymers.
CTE, linear, Transverse to Flow 100 µm/m-°C

@Temperature 20.0 °C
55.6 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
DSM Akulon® S223-E Nylon 66 (European and Asian Grade) (Dry)  (discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
CTE, linear, Transverse to Flow 100 µm/m-°C

@Temperature 23.0 - 55.0 °C
55.6 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 45HSB NC010 Nylon 66  (Unverified Data**)
Zytel® 45HSB NC010 is a high viscosity, heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-1/-2
Lanxess Pocan® BF 4130 XF 700051 PBT, 30% Glass Fiber
PBT, 30% glass fibers, injection molding, flame retardant, improved flowability
CTE, linear, Transverse to Flow 100 µm/m-°C

@Temperature 23.0 - 80.0 °C
55.6 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Valox® V9260CS PET (Europe-Africa-Middle East)
Color Stable Glass filled PET
CTE, linear, Transverse to Flow 100 µm/m-°C

@Temperature 23.0 - 55.0 °C
55.6 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2
Polyplastics Duranex® 3116 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 7.5% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
dry; ISO 11359-1/-2
DSM Akulon® F-X9215 PA6
Low/Medium Viscosity
CTE, linear, Transverse to Flow 100 µm/m-°C

@Temperature 20.0 °C
55.6 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
DSM Akulon® K224-LGM35 (Dry) 15% Glass Reinforced, 25% Mineral Reinforced Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
CTE, linear, Transverse to Flow 100 µm/m-°C

@Temperature 20.0 °C
55.6 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
DSM Akulon® S223-D Nylon 66 (European Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® BGZ-50/2 PA6-I-GF50
Information provided by EMS Grivory
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® BS/2 PA6
Product description: Grilon BS/2 is an unreinforced, nucleated standard PA6 injection molding grade with normal melt viscosity. Grilon BS/2 has the following important properties: Good flow behavior..
CTE, linear, Transverse to Flow 100 µm/m-°C

@Temperature 20.0 °C
55.6 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
DSM Stanyl® TW300 (DAM) Nylon 46 Heat Stabilized, Lubricated (North America)
Information provided by DSM Engineering Plastics.
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® TSG-35 PA666-GF35
Information provided by EMS Grivory
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-1/-2
DuPont Performance Polymers Delrin® 510GR NC000 Acetal (POM)  (Unverified Data**)
10% Glass Reinforced Medium Viscosity Acetal Homopolymer Delrin 510GR is a 10% glass reinforced acetal homopolymer for injection molding. It has high strength stiffness and high deflection temperatu..
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-1/-2
DuPont Performance Polymers Delrin® FG500TL NC010 Acetal (POM)  (Unverified Data**)
Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact ApplicationsDelrin FG500TL medium viscosity acetal homopolymer resin containing 1.5%..
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-2
Celanese CELANEX 3300D PBT, 30% Glass Reinforced
Celanex 3300D is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outsta..
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-2
Celanese CELANEX 3300HR PBT, 30% Glass Reinforced
Celanex 3300HR is a 30% glass reinforced polybutylene terephthalate which has excellent hydrolysis resistance, mechanical properties and processabilityInformation provided by Celanese
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-2
Celanese CELANEX 4202 PBT, 15% Glass Reinforced
Celanex 4202 is a 15% glass reinforced, impact modified polybutylene terephthalate with excellent surface appearance.Information provided by Celanese
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-2
Celanese Celcon® M90SW POM, Tribological
Celcon M90SW is a low wear grade designed for gears and other low wear applications, especially where reducing noise and wear against the same mating surface is important. This grade may be preferre..
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-2
Celanese CELANEX 4016 PBT, Unfilled
Non-exuding, unfilled, flame retardant polybutylene terephthalate which has an excellent balance of mechanical properties and processability. Celanex 4016 is well suited for applications requiring i..
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-2
Celanese Celcon® M50 POM, Unfilled
Celcon« M50 is a extrusion and injection molding grade with an intermediate viscosity for good processability with higher toughness than general purpose grades.Information provided by Celanese
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-2
Celanese Celcon® MR90B POM, Specialty
Celcon« MR90B is a standard flow specialty media resistant grade developed for improved bleach resistance.Information provided by Celanese
CTE, linear, Transverse to Flow 100 - 210 µm/m-°C
55.6 - 117 µin/in-°F
Average value: 169 µm/m-°C Grade Count:7
Overview of materials for Polyether Block Amide (PEBA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a..
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-2
Celanese Celanex® 3300D PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3300D is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outsta..