Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.10 GPa | 1170 ksi | conditioned, 1 mm/min; ISO 527-1,-2 |
Lanxess Durethan® AKV 35 LT H3.0 000000 Nylon 66, 35% Glass Fiber PA 66, 35% glass fiberInformation provided by LANXESS. |
|||
Tensile Modulus | 8.10 GPa | 1170 ksi | ISO 527-1/-2 |
Lanxess Durethan® BKV 230 H2.0 901510 Copolyamide, 30% Glass Fiber CoPA, injection molding grade, 30% glass fibers, elastomer-modified, higher impact and notched impact strength and also higher energy absorption under biaxial impact load than BKV 130, conditioning .. |
|||
Tensile Modulus | 8.10 GPa | 1170 ksi | |
LATI Latistat 62-06 K/10 PA6, 10% Carbon Fiber Reinforced Dissipative product based on Polyamide 6 (PA6). Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplasti.. |
|||
Tensile Modulus | 8.10 GPa | 1170 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP KFI16 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KFI16 is a compound based on Acetal Copolymer resin containing Glass Fiber, Silicone. |
|||
Tensile Modulus | 8.05 GPa | 1170 ksi | ISO 527 Type 1A |
Solvay TECHNYL® C 30H1 V30 Natural/F PA6, 30% glass fiber, Conditioned Description: Flame retardant polyamide PA6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This gr.. |
|||
Tensile Modulus | 8.10 GPa | 1170 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP QFP36 PA6.10 (Europe-Africa-Middle East) LNP* LUBRICOMP* QFP36 is a compound based on PA6.10 resin containg Glass Fiber, PTFE, Silicone. Added features include: Internally Lubricated. |
|||
Tensile Modulus | 8.06 GPa | 1170 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFL34 PA 66 LNP* LUBRICOMP* RFL34 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 8.06 GPa | 1170 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFL34 PA 66 (Asia Pacific) LNP* Lubricomp* RFL34 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 8.05 GPa | 1170 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® SHF434HR PBT PBT, Super High Flow, 20% glass reinforced,hydrolytically resistant. |
|||
Tensile Modulus | 8.10 GPa | 1170 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DF006 PC (Europe-Africa-Middle East) LNP* Thermocomp* DF1006 is a compound based on Polycarbonate resin containing Glass Fiber. |
|||
Tensile Modulus | 8.10 GPa | 1170 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RFB53XXZ PA 66 LNP* THERMOCOMP* RFB53XXZ is a compound based on Nylon 66 resin containing 15% Glass Fiber, 25% Glass Bead. |
|||
Tensile Modulus | 8.04 GPa | 1170 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DE003M PC LNP* STAT-KON* DE003M is a compound based on Polycarbonate containing 15% Milled Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
Tensile Modulus | 8.08 GPa | 1170 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP 2F006 ETFE LNP* THERMOCOMP* 2F006 is a compound based on ETFE containing 30% Glass Fiber. |
|||
Tensile Modulus | 8.10 GPa | 1170 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP MC004 PP (Europe-Africa-Middle East) LNP* Thermocomp* MC004 is a compound based on Polypropylene resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 8.10 GPa | 1170 ksi | ASTM D638 |
Plenco 2571 Phenolic, Granular, Transfer Molded PLENCO 02571 is a general purpose, organic filled phenolic molding compound offering optimum cure characteristics while maintaining excellent mechanical and electrical properties. UL recognized unde.. |
|||
Tensile Modulus | 8.10 GPa | 1170 ksi | ASTM D638 |
Plenco 4485 Phenolic, Granular, Injection Molded PLENCO 04485 is a mineral filled phenolic molding compound offering excellent heat resistance, electrical resistance, and dimensional stability. UL recognized under component file E40654. 04485 is a.. |
|||
Tensile Modulus | 8.10 GPa | 1170 ksi | ASTM D638 |
Plenco 7200 Phenolic, Granular, Transfer Molded PLENCO 07200 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength, good powder properties and excellent cosmetic properties. UL recognized under component .. |
|||
Tensile Modulus | 8.10 GPa | 1170 ksi | ASTM D638 |
Plenco 7500 Phenolic, Granular, Injection Molded PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi.. |
|||
Tensile Modulus | 8.10 GPa | 1170 ksi | ISO 527 |
Polyram RamSter PF305G6 PBT, 30% Glass Fiber 30% Glass fiber reinforced, PBT for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 8.10 GPa | 1170 ksi | ISO 527-2 |
Borealis Xmod™ GD301HP High Performance 32% Glass Fiber Reinforced Xmod GD301HP is reinforced with 32% chemically coupled glass fibers and based on specific Polymer matrix material which is bringing excellent mechanical properties (impact behavior) and very good st.. |
|||
Tensile Modulus | 8.10 GPa | 1170 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® RS 30G30HSL BK038A Nylon 610 30% Glass Reinforced Renewably Sourced Polyamide 610 Developed for Extrusion Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 8.10 GPa | 1170 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide AG5K PA66, 25% Glass Filled, Injection Molded AG5 is a Heat and Hydrolytically Stabilized, 25% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
Tensile Modulus | 8.10 GPa | 1170 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam PZ00062E PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX0062E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 8.10 GPa | 1170 ksi | ASTM D638 |
Plenco 7307 Phenolic, Granular, Transfer Molded PLENCO 07307 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength properties. Type ASTM 5948 CFG, and UL recognized under component file E40654. 07307 is a.. |
|||
Tensile Modulus | 8.10 GPa | 1170 ksi | |
LATI Latimass 37 B01-01 D025 Bio-Polymer Specific density compound based on Bio-Polymer (PLA, PHB, ...). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |