Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DFL36 PC LNP* LUBRICOMP* DFL36 is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin. Th.. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | ISO 180/U |
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos.. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DFL36 PC (Europe-Africa-Middle East) LNP* Lubricomp* DFL-4036 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. |
|||
Izod Impact, Unnotched (ISO) | 55.0 - 60.0 kJ/m² @Temperature -30.0 - -30.0 °C |
26.2 - 28.6 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 57.5 kJ/m² Grade Count:2 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1U |
Lanxess Pocan® KU 2-7241 000000 PBT, 25% Glass Fiber PBT, 25% glass fibers, injection molding, flame retardant, improved impact strengthInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP QFP36 PA6.10 (Europe-Africa-Middle East) LNP* LUBRICOMP* QFP36 is a compound based on PA6.10 resin containg Glass Fiber, PTFE, Silicone. Added features include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRILOY RF208 PA 66 LNP LUBRILOY* RF208 is a compound based on Nylon 66 resin containing 40% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® 4031 PBT (Europe-Africa-Middle East) VALOX 4031 is a 30% high strength glass fibre reinforced PBT injection moulding resin with excellent strength, stiffness and heat resistance. Applications: appliance handles, spotlights, electric mo.. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® 4031 PBT (Europe-Africa-Middle East) VALOX 4031 is a 30% high strength glass fibre reinforced PBT injection moulding resin with excellent strength, stiffness and heat resistance. Applications: appliance handles, spotlights, electric mo.. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP DF003E PC (Asia Pacific) LNP* Thermocomp* DF003E is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP DF004ER PC (Europe-Africa-Middle East) LNP* Thermocomp* DF004ER is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RF007H PA 66 LNP* Thermocomp* RF007H is a compound based on Nylon 66 containing glass fiber. Added feature includes: Healthcare. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RF007SXP PA 66 LNP* THERMOCOMP* RF007SXP is a compound based on Nylon 66 containing 35% Glass Fiber. Added feature of this material includes: Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP UF008AR PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UF008AR is a compound based on Polyphthalamide resin, containing Glass Fiber. Added features include; Mold Release. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP UX06028 PPA (Europe-Africa-Middle East) LNP * THERMOCOMP* UX06028 is a compund based on Polyphthalamide resin, containing Glass Fiber. Added features include Mold Release. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON MV00AS PP (Europe-Africa-Middle East) LNP VERTON* MV00AS is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled, heat stabilized |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s.. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA (Asia Pacific) Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s.. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP IP004Z PA6.12 (Europe-Africa-Middle East) LNP* LUBRICOMP* IP004Z is a compound based on PA 6/12 resin containing PTFE, Silicone. Added features include : Internally Lubricated, Extrusion grade. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp RFC16 PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RFC16 is a compound based on PA 66 resin containing Glass Fiber, Carbon Fiber. Added features include: Easy Molding.This data was supplied by SABIC-IP for the Europe-Africa-Middle.. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL 731 PPE+HIPS (Asia Pacific) PPE+PS, HDT 125 |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Staramide PF007IX2 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide PF007IX1 is an Impact Modified, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as Star X 2010 33V)Information provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Staramide RFC16 PA66/6, Glass/Carbon Fiber Filled, Injection Molded RFC16 is a Glass Fiber and Carbon Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as STAR C PA66 C 303VY Z3)Information provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starflam RF0077E PA66, 35% Glass Filled, Injection Molded Starflam RF0077E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding Resin (also known as RF1007Z270)Information provided by Polymer T.. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | ISO 180/1C |
Chi Mei Polylac® PA-758R ABS - Transparent Transparent, Chemical Resistant |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | ASTM D256 |
Beijing Ranger Chem PBT-201-G20 211 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | ASTM D256 |
Beijing Ranger Chem PBT-201-G25 291 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | ASTM D256 |
BLUESTAR 201-G25202 PBT, 25% Glass Filled Typical Applications: Energy saving lighting, E/E applicationsInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | ASTM D256 |
Beijing Ranger Chem PBT-201-G0 211 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |