Fainplast Compounds FK 90/1 Flexible PVC, Insulation Lead Free

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Fainplast Compounds
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds FK 90/1 Flexible PVC, Insulation Lead Free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Oil resistant insulation
Physical Properties Metric English Comments
Density 1.40 - 1.44 g/cc
0.0506 - 0.0520 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 88 - 92
88 - 92
ISO R 868
Tensile Strength at Break >= 19.0 MPa
>= 2760 psi
ISO R 527
Elongation at Break >= 340 %
>= 340 %
ISO R 527
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+14 ohm-cm

@Temperature 23.0 °C
3.00e+14 ohm-cm

@Temperature 73.4 °F
ASTM D257
Descriptive Properties Value Comments
Thermal Stability (minutes) 60
CEI 20-34/3-2