Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 23.0 µm/m-°C @Temperature 20.0 °C |
12.8 µin/in-°F @Temperature 68.0 °F |
ISO data |
BASF Capron® GR630 30% Glass-Filled Nylon 66 (Dry)
(discontinued **) Capron GR630 is a 30% glass fiber reinforced polyamide 6,6 injection molding compound offering excellent strength, stiffness, creep resistance and dimensional stability. This balance of engineering.. |
|||
CTE, linear, Parallel to Flow | 23.0 µm/m-°C @Temperature 20.0 °C |
12.8 µin/in-°F @Temperature 68.0 °F |
ISO data |
BASF Capron® 5233G HS BK-102 33% Glass-Filled Nylon 66 (Dry)
(discontinued **) Capron 5233G HS BK-102 is a 35% glass reinforced, heat stabilized, pigmented black nylon 6,6 injection molding compound offering excellent strength, rigidity, stiffness, creep resistance, and dimens.. |
|||
CTE, linear, Parallel to Flow | 23.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
12.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
|
Idemitsu Kosan Xarec® WA 552 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled/Impact Modified. Used in Automotive and Industrial applications. NSF and medical approval ISO 10993 |
|||
CTE, linear, Parallel to Flow | 23.0 µm/m-°C | 12.8 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® DP 2131/20 H2.0 900051 Nylon 6, 20% Glass Fiber PA 6, injection molding grade, 20% glass fibers, better surface resistance to alcoholic calcium chloride-solution than BKV 20 H2.0, good heat-ageing resistance and weather resistance |
|||
CTE, linear, Parallel to Flow | 23.0 µm/m-°C @Temperature 23.0 - 85.0 °C |
12.8 µin/in-°F @Temperature 73.4 - 185 °F |
ISO 11359 |
Solvay TECHNYL® SSD 330 KNF/E PA66, 15% glass filled, DRY Description: Polyamide 66, reinforced with 33% of glass fiber, for injection molding specially stabilized to improves its resistance to automotive cooling liquids.Available in: Asia PacificProduct A.. |
|||
CTE, linear, Parallel to Flow | 23.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
12.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36S PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFL36S is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 23.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
12.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP RFN1ASXS PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFN1ASXS is a compound based on Nylon 66 resin containing Glass Fiber, MOS2. Added features of this material include: Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 23.0 µm/m-°C @Temperature 23.0 - 150 °C |
12.8 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2312 PEI (Europe-Africa-Middle East) 30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
CTE, linear, Parallel to Flow | 23.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
12.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON RX06001 PA 66 (Europe-Africa-Middle East) LNP* Stat-kon* RX06001 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Easy Molding, High Impact, Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 23.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
12.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP AF006XXZ ABS (Europe-Africa-Middle East) LNP* Thermocomp* AF006XXZ is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 23.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
12.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP DX06094 PC (Europe-Africa-Middle East) LNP* THERMOCOMP* DX06094 is a compound based on Polycarbonate resin containing Glass Fiber . Added features include: High Impact, Non- Brominated & Non-Chlorinated Flame Retardant and Mold Release... |
|||
CTE, linear, Parallel to Flow | 23.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
12.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP UF008AR PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UF008AR is a compound based on Polyphthalamide resin, containing Glass Fiber. Added features include; Mold Release. |
|||
CTE, linear, Parallel to Flow | 23.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
12.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP UF008AS PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UF008AS is a compound based on Polyphthalamide resin, containing Glass Fiber. Added features include; Mold Release. |
|||
CTE, linear, Parallel to Flow | 23.0 µm/m-°C @Temperature 23.0 °C |
12.8 µin/in-°F @Temperature 73.4 °F |
TMA |
Sumitomo Bakelite North America RX® 660 Fiberglass Reinforced Phenolic Novolac RX 660 is a fiberglass reinforced phenolic molding compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type MFH.Information supplied by Sumitom.. |
|||
CTE, linear, Parallel to Flow | 23.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
12.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP VERTON MV00ES PP LNP* VERTON* MV00ES is primarily a concentrate used for blending purposes. This is a 70% long glass fiber Polypropylene compound. Added features of this grade are: Heat Stabilized |
|||
CTE, linear, Parallel to Flow | 23.0 µm/m-°C @Temperature 23.0 - 85.0 °C |
12.8 µin/in-°F @Temperature 73.4 - 185 °F |
ISO 11359 |
Solvay TECHNYL® A 216T V33 Black 1 N PA66, 33% glass fiber, DRY Description: Polyamide PA66 reinforced with 33% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, EuropeProduct Applications: TECHNYL® A 216T V33 BLACK 1N is used.. |
|||
CTE, linear, Parallel to Flow | 23.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
12.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PCN2615H PPE+PS (Asia Pacific) PPE+PS, Noryl, Glass Fiber, Mica, Flame Retardant, UL Grade, Non-Halogen Flame Retaardant, High Flow, |
|||
CTE, linear, Parallel to Flow | 23.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
12.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON AE002 ABS (Europe-Africa-Middle East) LNP* STAT-KON* AE002 is a compound based on Acrylonitrile Butadiene Styrene resin containg Carbon Fiber. Added features include: Electrically Conductive |
|||
CTE, linear, Parallel to Flow | 23.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
12.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp EF006R PEI (Europe-Africa-Middle East) LNP* Thermocomp* EF006R is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Mold Release.This data was supplied by SABIC-IP for the Europe-A.. |
|||
CTE, linear, Parallel to Flow | 23.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
12.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp LF004 PEEK (Europe-Africa-Middle East) LNP* THERMOCOMP* LF004 Is a compound based on Polyetheretherketone containg Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 23.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
12.8 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® RE19051 BK507 Polyethylene Terephthalate (PET) 40% Glass/Mineral Reinforced Flame Retardant Polyethylene Terephthalate Rynite RE19051 BK507 is a 40% glass and mineral reinforced flame retardant polyethylene terephthalate black resin.Information .. |
|||
CTE, linear, Parallel to Flow | 23.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
12.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starflam RF0069 PA66, 30% Glass Fiber, Flame Retardant, Injection Molded Starflam RF0069 is a Flame Retardant, 30% Glass Reinforced Polyamide 66 Injection Molding Resin (also known as PA66 30V U2 Z79 or RF1006Z590)Information provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 23.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
12.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starflam AFR460B PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR460B is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 23.0 µm/m-°C | 12.8 µin/in-°F | ASTM Test |
BASF Petra® 130 30% Glass Filled PET Petra 130 is a 30% glass fiber reinforced polyethylene terephthalate (PET) for injection molding applications. It exhibits a good combination of performance properties including high strength and s.. |
|||
CTE, linear, Parallel to Flow | 23.0 µm/m-°C @Temperature 20.0 °C |
12.8 µin/in-°F @Temperature 68.0 °F |
ISO data |
BASF Capron® GR630 HS 30% Glass-Filled Nylon 66 (Dry)
(discontinued **) Capron GR630 HS is a heat stabilized, 30% glass fiber reinforced polyamide 6,6 injection molding compound offering excellent strength, stiffness, creep resistance and dimensional stability. This ba.. |
|||
CTE, linear, Parallel to Flow | 23.0 µm/m-°C @Temperature 20.0 °C |
12.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit X611 Novolac Phenolic Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties. UL listed.USES: Complex precision parts with thin cross section and good mechanical properties e.g. in.. |
|||
CTE, linear, Parallel to Flow | 23.0 µm/m-°C @Temperature 20.0 °C |
12.8 µin/in-°F @Temperature 68.0 °F |
ASTM E-831 |
Sumitomo Bakelite North America RX® 852 Novolac Phenolic Fiberglass reinforced phenolic novolac compound with good dimensional stability and good strength at elevated temperatures.Information provided by Vyncolit, a Sumitomo Bak Group |