Trelleborg Emerson & Cuming Eccobond® 83C Two-Component Silver Filled Electrically Conductive Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive , Epoxy, Electrically Conductive
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name Eccobond®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Emerson & Cuming Eccobond® 83C Two-Component Silver Filled Electrically Conductive Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Emerson & Cuming 83C Eccobond® Two-Component Silver Filled Electrically Conductive Epoxy AdhesiveTwo component, silver filled, electrically conductive, epoxy adhesive. Smooth, creamy consistency. Good thermal conductivity. Requires heat cure to obtain optimal properties. Easier handling version of Eccobond® 56C with similar properties. Mix ratio of 100:3.5. Cure Type: Heat Bonding Type: Epoxy
Physical Properties Metric English Comments
Density 3.00 g/cc
0.108 lb/in³
Mechanical Properties Metric English Comments
Adhesive Bond Strength 6.89 MPa
1000 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 0.00040 ohm-cm
0.00040 ohm-cm
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 100 °C
0.500 hour

@Temperature 212 °F
60.0 min

@Temperature 65.0 °C
1.00 hour

@Temperature 149 °F
Descriptive Properties Value Comments
Color Silver
Viscosity Thixotropic (Mixed, 25°C)