Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-2
Celanese Celanex® 3309HRLM PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3309HRLM is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and processability.30% glass filled PBT, h..
CTE, linear, Transverse to Flow 100 µm/m-°C

@Temperature 23.0 - 55.0 °C
55.6 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 45HSB NC010 Nylon 66  (Unverified Data**)
Zytel® 45HSB NC010 is a high viscosity, heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-1/-2
Lanxess Durethan® AKV 325 H2.0 901510 Nylon 66, 25% Glass Fiber
PA 66, 25% glass fibers, extrusion- and blow molding grade, branched, high viscosity, good heat-ageing resistance, good hydrolysis resistance
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-1/-2
Lanxess Pocan® KU 2-7205 000000 PBT
PBT, non-reinforced, injection molding, extrusion, flame retardant
CTE, linear, Transverse to Flow 100 µm/m-°C

@Temperature 23.0 - 55.0 °C
55.6 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1, -2
Lanxess Durethan® BKV 30 H2.0 EF 000000 Nylon 6, Glass Fiber Reinforced
PA 6, 30% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS.
CTE, linear, Transverse to Flow 100 µm/m-°C

@Temperature 23.0 - 60.0 °C
55.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP RFL22E PA6.6 (Europe-Africa-Middle East)
LNP* LUBRICOMP* RFL22E Is a compound based on PA66 resin, containing Glass Fiber and PTFE. Added features include: Internally Lubricated, Easy Moulding
CTE, linear, Transverse to Flow 100 µm/m-°C

@Temperature 23.0 - 60.0 °C
55.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP RN001 PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RN001 is a compound based on Nylon 66 resin containing MOS2.
CTE, linear, Transverse to Flow 100 µm/m-°C

@Temperature -40.0 - 40.0 °C
55.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® SHF4340 PBT (Europe-Africa-Middle East)
20% GF Super High Flow PBT
CTE, linear, Transverse to Flow 100 µm/m-°C

@Temperature 23.0 - 80.0 °C
55.6 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Valox® V9260CS PET (Asia Pacific)
Color Stable Glass filled PET
CTE, linear, Transverse to Flow 100 µm/m-°C

@Temperature 23.0 - 80.0 °C
55.6 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Noryl HF180 PPE+HIPS (Europe-Africa-Middle East)
NORYL HF180 is an unfilled, flame retardant material with a Vicat B/120 of 100°C according ISO 306. NORYL HF180 is V1 at 2.0 mm according UL94 and halogenThis data was supplied by SABIC-IP for th..
CTE, linear, Transverse to Flow 100 µm/m-°C

@Temperature 23.0 - 80.0 °C
55.6 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics NORYL ENV105 PPE+HIPS (Europe-Africa-Middle East)
NORYL ENV105 is an impact modified extrusion grade with a Vicat B/120 of 115C according ISO 306.
CTE, linear, Transverse to Flow 100 µm/m-°C

@Temperature 23.0 - 55.0 °C
55.6 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2
Polyplastics Duranex® 3226 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 20% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® XE 4071 black 9992 PA612
Product description: Grilamid XE 4071 BLACK 9992 is an impact modified unreinforced high viscosity polyamide 612 (PA612) extrusion grade with superior heat and hydrolysis resistance. Compared to sta..
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® XE 4071 nat PA612-I
Product description: Grilamid XE 4071 NATURAL is an unreinforced impact modified high viscosity polyamide 612 (PA612) extrusion grade with superior hydrolysis and heat resistance. Compared to standa..
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-1/-2
DuPont Performance Polymers Delrin® 911DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Low Viscosity Acetal Homopolymer Delrin 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less shrinka..
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® FR50 NC010A Nylon 66  (Unverified Data**)
25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR50 NC010A is a 25% glass fiber reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performanc..
CTE, linear, Transverse to Flow 100 µm/m-°C

@Temperature 23.0 - 60.0 °C
55.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide AG3X3 PA66, Glass Fiber Reinforced, Impact Modified, Injection Molding
Staramide AG3X3 is an Impact Modified, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-1/-2
DuPont Performance Polymers Delrin® 100KM NC000 Acetal (POM)  (Unverified Data**)
Kevlar® Modified High Viscosity Acetal Homopolymer with Low Wear and Low FrictionDelrin 100KM is a high viscosity acetal homopolymer resin modified with Kevlar aramid resin. It is designed for appl..
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-2
Celanese CELANEX 2008 PBT, Unfilled
Celanex 2008 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in melt blown applications.Information provided by ..
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-2
Celanese Hostaform® LX90Z XAP2 ™ POM, UV Resistant
Preliminary Data SheetDrying is required for this material to prevent poor appearance and performance of the part.Information provided by Celanese Corporation.
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-2
Celanese CELANEX 3300-2FC PBT, 30% Glass Reinforced
Celanex 3300-2FC is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outs..
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-2
Celanese Celanex® 3309HRHF PBT, 30% Glass Reinforced
Celanex 3309HRHF is a 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and improved flow.Information provided by Celanese Corpora..
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-2
Celanese IMPET 2700 GV1/45 (Europe) PET, 45% Glass Reinforced
Polyethylene terephthalate, 45 % glass filled, high flowability, excellent gloss, high modulus, very high heat deflection temperature.Information provided by Celanese
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-2
Celanese THERMX LED 0201S PCT, 38% Specialty
Thermx LED 0201S is a super white reinforced PCT resin highly suitable for LED applications. The material exhibits high heat resistance, high reflectance stability, high thermal stability, low mois..
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-1/-2
DuPont Performance Polymers Crastin® LW9020FR NC010 PBT+ASA  (Unverified Data**)
20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020FR NC010 is a 20% glass fiber reinforced flame retardant polybutylene terephthal..
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-2
Celanese Celcon® GC15 POM, 15% Glass Reinforced  (Unverified Data**)
Celcon® GC15 is an acetal copolymer grade utilizing a nominal 15 wt. % fiber glass level to increase stiffness and strength.15% glass fibers, coupled for improved stiffnessStandard reciprocating sc..
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-2
Celanese Hostaform® CP15X POM  (Unverified Data**)
Preliminary Data Sheetcreep resistant, high viscosity acetal copolymerInformation provided by Celanese
CTE, linear, Transverse to Flow 100 µm/m-°C

@Temperature 23.0 - 55.0 °C
55.6 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2
Polyplastics Duracon® CH-10 Acetal Co-polymer (POM), Conductive, CF reinforced, Wear resistance
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..