LG Chemical DOA Plasticizer

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer LG Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical DOA Plasticizer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: LG DOA is an aliphatic plasticizer and used to keep softness of product under cold water.Application: Wrap for food package, synthetic leather, sheet, hose, gasketInformation provided by LG Chemical
Physical Properties Metric English Comments
Viscosity 11 cP
11 cP
Molecular Weight 317 g/mol
317 g/mol
Thermal Properties Metric English Comments
Melting Point -70.0 °C
-94.0 °F
Freezing Point
Boiling Point 335 °C
635 °F
Flash Point 196 °C
385 °F
Chemical Properties Metric English Comments
Acid Value <= 0.10

@Treatment Temp. 125 °C,
Time 10800 sec
<= 0.10

@Treatment Temp. 257 °F,
Time 3.00 hour
After Heating, KOH mg/g; JIS K6751
Descriptive Properties Value Comments
Acidity <0.03 KOH mg/g
JIS K6751
Color <15 APHA
JIS K6751
Ester Value 299-305
JIS K6751
Heat Loss <0.1%
125°Cx3hr, JIS K6751