Quadrant EPP Ketron® HPV PEEK + carbon fibres + PTFE + graphite, bearing grade, extruded (ISO Data)

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled
Manufacturer Quadrant Engineering Plastics Products
Trade Name Ketron®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Ketron® HPV PEEK + carbon fibres + PTFE + graphite, bearing grade, extruded (ISO Data).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The addition of carbon fibres, PTFE and graphite to virgin PEEK results in a Ketron PEEK “bearing grade”. Its excellent tribological properties (low friction, long wear and high pressure-velocity capabilities) make this grade especially suited for wear and friction applications. Very high maximum allowable service temperature in air (250 °C continuously, up to 310 °C for short periods of time) High mechanical strength, stiffness and creep resistance, also at elevated temperatures Excellent chemical and hydrolysis resistance Excellent wear & frictional behaviour Very good dimensional stability Excellent resistance to high energy radiation (gamma- and X-rays) Inherent low flammability and very low levels of smoke evolution during combustion
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183-1
Moisture Absorption at Equilibrium 0.16 %
0.16 %
50% RH
Water Absorption at Saturation 0.35 %
0.35 %
Outgassing - Total Mass Loss 0.16 %
0.16 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 85
85
ISO 2039-2
Hardness, Shore D 86
86
Ball Indentation Hardness 215 MPa
31200 psi
ISO 2039-1
Tensile Strength 78.0 MPa
11300 psi
at Break (NYP); ISO 527-1/-2
Elongation at Break 3.0 %
3.0 %
ISO 527-1/-2
Tensile Modulus 5.90 GPa
856 ksi
ISO 527-1/-2
Flexural Strength 125 MPa
18100 psi
Compressive Strength 46.0 MPa

@Strain 1 %
6670 psi

@Strain 1 %
ISO 604
80.0 MPa

@Strain 2 %
11600 psi

@Strain 2 %
ISO 604
120 MPa

@Strain 5 %
17400 psi

@Strain 5 %
ISO 604
K Factor (ISO) 2.0 µm/km
2.0 µm/km
Charpy Impact Unnotched 2.50 J/cm²
11.9 ft-lb/in²
ISO 179-1/1eU
Charpy Impact, Notched 0.300 J/cm²
1.43 ft-lb/in²
ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.15 - 0.25
0.15 - 0.25
Limiting Pressure Velocity 0.420 MPa-m/sec
12000 psi-ft/min
at 1 m/s unlubricated
0.660 MPa-m/sec
18800 psi-ft/min
at 0.1 m/s unlubricated
Thermal Properties Metric English Comments
CTE, linear 35.0 µm/m-°C

@Temperature 23.0 - 100 °C
19.4 µin/in-°F

@Temperature 73.4 - 212 °F
Thermal Conductivity 0.780 W/m-K
5.41 BTU-in/hr-ft²-°F
Melting Point 340 °C
644 °F
DSC, 10°C/min.; ISO 11357-1/-3
Maximum Service Temperature, Air 250 °C
482 °F
Continuous
Deflection Temperature at 1.8 MPa (264 psi) 195 °C
383 °F
ISO 75-1/-2
Flammability, UL94 V-0
V-0
Oxygen Index 43 %
43 %
ISO 4589-1/-2
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 1e+13 ohm
<= 1e+13 ohm
IEC 60093
Compliance Properties Metric English Comments
3A-Dairy No
No
European Food 1935/2004 No
No
FDA No
No
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Limited
Limited
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Acceptable
Alkalies, Weak Acceptable
Acceptable
Chlorinated Solvents Acceptable
Acceptable
Continuous Sunlight Acceptable
Acceptable
Hot Water / Steam Acceptable
Acceptable
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable
Users viewing this material also viewed the following: