Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 340 °C | 644 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Ketron® 1000 IM Injection Molded Unfilled Polyetheretherketone (ASTM Product Data Sheet) Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to hot water or steam |
|||
Melting Point | 340 °C | 644 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Ketron® 1000 LSG PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Datasheet) |
|||
Melting Point | 340 °C | 644 °F | ISO 11357 |
Quadrant EPP Ketron® CA30 LSG PEEK, Extruded 30% Carbon Fiber Reinforced Polyetherether Ketone (ASTM Product Data Sheet) |
|||
Melting Point | 340 °C | 644 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Ketron® CA30 PEEK, Extruded 30% Carbon Fiber Reinforced Polyetherether Ketone (ASTM Product Data Sheet) |
|||
Melting Point | 340 °C | 644 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Ketron® CM GF30 Compression Molded, 30% Glass Reinforces Polyethererther Ketone(ASTM Product Data Sheet) |
|||
Melting Point | 340 °C | 644 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Ketron® CM HPV PEEK Polyetheretherketone; PTFE, Graphite, and Carbon Fiber Filled Bearing Grade, compression molded (ASTM Product Data Sheet) Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to hot water or steam |
|||
Melting Point | 340 °C | 644 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
Quadrant EPP Ketron® HPV PEEK + carbon fibres + PTFE + graphite, bearing grade, extruded (ISO Data) The addition of carbon fibres, PTFE and graphite to virgin PEEK results in a Ketron PEEK “bearing grade”. Its excellent tribological properties (low friction, long wear and high pressure-velocity .. |
|||
Melting Point | 340 °C | 644 °F | ASTM D3418 |
Quadrant EPP KETRON® MD PEEK, A Metal-Detectable Polyetheretherketone |
|||
Melting Point | 340 °C | 644 °F | Peak (major component); ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been formula.. |
|||
Melting Point | 340 °C | 644 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stability.. |
|||
Melting Point | 340 °C | 644 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gr.. |
|||
Melting Point | 340 °C | 644 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire PEEK is produced to the highest industry standards and is characteriz.. |
|||
Melting Point | 340 °C | 644 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical prope.. |
|||
Melting Point | 340 °C | 644 °F | ASTM D3417 |
Solvay Specialty Polymers KetaSpire® KT-820FP Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820FP is the low-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color fine powder form suitable for compression molding. KetaSpire PEEK is produced to the .. |
|||
Melting Point | 340 °C | 644 °F | ASTM D3417 |
Solvay Specialty Polymers KetaSpire® KT-820P Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820P is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire PEEK is produced to the highest industry standards and is .. |
|||
Melting Point | 340 °C | 644 °F | ASTM D3417 |
Solvay Specialty Polymers KetaSpire® KT-850P Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-850P is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire PEEK is produced to the highest industry standa.. |
|||
Melting Point | 340 °C | 644 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro.. |
|||
Melting Point | 340 °C | 644 °F | ASTM D3418 |
Quadrant EPP Ketron® GF30 LSG PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone (ASTM Product Data Sheet) |
|||
Melting Point | 340 °C | 644 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Semitron® ESd 490HR Static dissipative PEEK for use in test fixtures. Non-sloughing and low moisture absorption. (ASTM Product Data Sheet) |
|||
Melting Point | 340 °C | 644 °F | ASTM D3418 |
Solvay Specialty Polymers Ajedium™ KT-820 Polyetheretherketone (PEEK) KetaSpire® KT-820 PEEK film is thermoplastic film that is characterized by a distinct combination of properties, which include excellent wear resistance, best-in-class fatigue resistance, high pu.. |
|||
Melting Point | 340 °C | 644 °F | ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire® AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This r.. |
|||
Melting Point | 340 °C | 644 °F | ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining.. |
|||
Melting Point | 340 °C | 644 °F | ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparabl.. |
|||
Melting Point | 340 °C | 644 °F | ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK) AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stabi.. |
|||
Melting Point | 340 °C | 644 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-820FP Polyetheretherketone (PEEK) KetaSpire® KT-820FP is the low-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color fine powder form suitable for compression molding. KetaSpire® PEEK is produced.. |
|||
Melting Point | 340 °C | 644 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-820P Polyetheretherketone (PEEK) KetaSpire® KT-820P is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire® PEEK is produced to the highest industry standards.. |
|||
Melting Point | 340 °C | 644 °F | DSC |
Wolf Kunststoff ZEDEX® ZX-324V1T A3H PEEK Polymer, Reinforced Main Characteristics: High resilience; High elasticity; Low permanent deformation; Stress resistant; High strength at temperatures above 140 ° CApplications: Shipbuilding; Chemical Engineering; Aut.. |
|||
Melting Point | 340 °C | 644 °F | DSC |
Wolf Kunststoff ZEDEX® ZX-324V2T A3F PEEK, PTFE Modified Reduced friction; High wear resistance; High elasticity; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automotive Technology; Machine ToolsInformation provided by Zedex |
|||
Melting Point | 340 °C | 644 °F | ISO 11357-1 |
Murtfeldt Murpec® SP Polyetheretherketone Modified Murpec® SP provides excellent slide properties in addition to good mechanical properties. Murpec® SP also offers improved wear behavior due to its special additives.Special Properties:• .. |
|||
Melting Point | 340 °C | 644 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
Quadrant EPP Ketron® GF30 PEEK + glassfibres, extruded (ISO Data) This 30 % glass fibre reinforced grade offers a higher stiffness and creep resistance than Ketron PEEK-1000 and has a much better dimensional stability. This grade is very appropriate for structural.. |