Mechanical Properties Metric English Comments
Ball Indentation Hardness 215 MPa
31200 psi
ISO 2039-1
Quadrant EPP Ketron® HPV PEEK + carbon fibres + PTFE + graphite, bearing grade, extruded (ISO Data)
The addition of carbon fibres, PTFE and graphite to virgin PEEK results in a Ketron PEEK “bearing grade”. Its excellent tribological properties (low friction, long wear and high pressure-velocity ..
Ball Indentation Hardness 215 - 440 MPa
31200 - 63800 psi
Average value: 323 MPa Grade Count:4
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu..
Ball Indentation Hardness 215 MPa
31200 psi
ISO 2039-1
Quadrant EPP Ketron® GF30 LSG PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone (ASTM Product Data Sheet)
Ball Indentation Hardness 215 MPa
31200 psi
dry; ISO 2039-1
EMS-Grivory Grivory® GVN-35H black 9915 PA*-GF35
Product description: Grivory GVN-35H is a 35% glass-fiber reinforced, impact-modified engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic c..
Ball Indentation Hardness 215 MPa
31200 psi
dry; ISO 2039-1
EMS-Grivory Grivory® XE 4104 black 9992 PA610-GF40
Product description: Grilamid XE 4104 black 9992 is a 40% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mate..
Ball Indentation Hardness 215 MPa
31200 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® XE 4116 black 9288 PA1010-GF55
Product description: Grilamid XE 4116 black 9288 is a 55% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is especially suitable for the manufacturing of thin-walled, paint..
Ball Indentation Hardness 215 MPa
31200 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® XE 4116 nat PA1010-GF55
Product description: Grilamid XE 4116 natural is a 55% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is especially suitable for the manufacturing of thin-walled, painted ..
Ball Indentation Hardness 215 MPa
31200 psi
H 961/30; ISO 2039-1
Akro-Plastic Akromid® B3 GF 25 (2471) PA 6 Dry, 25% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
Ball Indentation Hardness 215 MPa
31200 psi
ISO 2039-1
Murtfeldt Murpec® SP Polyetheretherketone
Modified Murpec® SP provides excellent slide properties in addition to good mechanical properties. Murpec® SP also offers improved wear behavior due to its special additives.Special Properties:• ..