Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.780 W/m-K | 5.41 BTU-in/hr-ft²-°F | |
Quadrant EPP Ketron® HPV PEEK + carbon fibres + PTFE + graphite, bearing grade, extruded (ISO Data) The addition of carbon fibres, PTFE and graphite to virgin PEEK results in a Ketron PEEK “bearing grade”. Its excellent tribological properties (low friction, long wear and high pressure-velocity .. |
|||
Thermal Conductivity | 0.780 W/m-K | 5.41 BTU-in/hr-ft²-°F | |
Schott F2 Glass Information Provided by SCHOTT North America, Inc. |
|||
Thermal Conductivity | 0.780 W/m-K | 5.41 BTU-in/hr-ft²-°F | |
Schott F2HT Glass Information Provided by SCHOTT North America, Inc. |
|||
Thermal Conductivity | 0.780 W/m-K | 5.41 BTU-in/hr-ft²-°F | |
Schott N-BAF10 Glass Information Provided by SCHOTT North America, Inc. |
|||
Thermal Conductivity | 0.780 W/m-K | 5.41 BTU-in/hr-ft²-°F | Moulding Direction; ASTM C177 |
Dalau Dalcon 018 85% Virgin PTFE, 15% Graphite Applications & Industries: General: Graphite filler improves the sliding properties & thermal conductivity of PTFE and has one of the lowest coefficient of frictions. It has low wear in water and is.. |
|||
Thermal Conductivity | 0.780 W/m-K @Temperature 121 °C |
5.41 BTU-in/hr-ft²-°F @Temperature 250 °F |
|
Tra-Con Tra-Bond 342-14T Low Viscosity Room Temperature Cure Epoxy Adhesive TRA-BOND 342-14T single component, low viscosity alumina-filled epoxy adhesive exhibits high bond strength and excellent thermal shock characteristics. This adhesive may be cured at room temperature.. |
|||
Thermal Conductivity | 0.780 W/m-K | 5.41 BTU-in/hr-ft²-°F | Moulding Direction; ASTM C177 |
Dalau Dalcon 018 85% Virgin PTFE, 15% Graphite Applications & Industries: General: Graphite filler improves the sliding properties & thermal conductivity of PTFE and has one of the lowest coefficient of frictions. It has low wear in water and is.. |
|||
Thermal Conductivity | 0.780 W/m-K @Temperature 50.0 °C |
5.41 BTU-in/hr-ft²-°F @Temperature 122 °F |
|
3M XLD3000 Glass Bubbles 3M™ Glass Bubbles XLD3000 are high-strength additives for polymers made from a water-resistant and chemically stable soda-lime-borosilicate glass. These hollow glass bubbles can be compounded with .. |