Polymer Property : Tensile Strength = 78.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 78.0 MPa
11300 psi
at Yield; ISO 527-1/-2
Quadrant EPP Ertacetal® H POM-H, extruded (ISO Data)
Ertacetal H is Quadrant’s homopolymer acetal grade. It offers a higher mechanical strength, stiffness, hardness and creep resistance as well as a lower thermal expansion rate and often also a bette..
Tensile Strength 78.0 MPa
11300 psi
at Break (NYP); ISO 527-1/-2
Quadrant EPP Ketron® HPV PEEK + carbon fibres + PTFE + graphite, bearing grade, extruded (ISO Data)
The addition of carbon fibres, PTFE and graphite to virgin PEEK results in a Ketron PEEK “bearing grade”. Its excellent tribological properties (low friction, long wear and high pressure-velocity ..
Tensile Strength 78.0 MPa
11300 psi
at Break (NYP); ISO 527-1/-2
Quadrant EPP Techtron® HPV PPS + solid lubricant, bearing grade, extruded (ISO Data)
As a reinforced, internally lubricated PPS grade, Techtron HPV PPS demonstrates an excellent combination of properties including wear resistance, load-bearing capabilities and dimensional stability ..
Tensile Strength 78.0 MPa
11300 psi
50 mm/min; ISO 527-1
Sax Polymers SAXAMID 126K6 Nylon 6, 30% Glass Filled
SAXAMID 126K6 is a 30% glass beads filled polyamide 6 injection-molding-grade. It is characterized by dimensional stability, low warpage and good surface quality.Information provided by SAX Polymers..
Tensile Strength 78.0 MPa
11300 psi
DIN EN ISO 527
Wolf Kunststoff ZEDEX® ZX-100K A1K Polymer Alloy
Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good weather resistance; Good machinability; FDA compliant LABS; PTFE and silicone-free; KTW approved; Stress resistantApplications: ..
Tensile Strength 78.0 MPa
11300 psi
cond.; ISO 527
Azoty Tarnow™ Tarnamid® T-27 GF10 MX10 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grade, reinforced with 10% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning, good surface quality.T..
Tensile Strength 78.0 MPa

@Strain 12.0 %,
Temperature 23.0 °C
11300 psi

@Strain 12.0 %,
Temperature 73.4 °F
50 mm/min; ISO 527-2
BASF Elastollan R 3000 20% Glass Filled TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan..
Tensile Strength 78.0 MPa

@Strain 8.00 %,
Temperature 23.0 °C
11300 psi

@Strain 8.00 %,
Temperature 73.4 °F
50 mm/min; ISO 527-2
BASF Elastollan R 3000 20% Glass Filled TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan..
Tensile Strength 78.0 MPa
11300 psi
5 mm/min; ISO 527-1
Sax Polymers SAXALEN PPH304G25 Polypropylene Homopolymer, 25% Glass Filled