Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 340 °C | 644 °F | |
Oceanchem Group Decabromodiphenyl Ethane (DBDPE/8010) Molecular Formula: C14Br10H4Cas No.: 84852-53-9Characteristics: White powder, no poison, no smell and noncorrosion. Indissolvable in water, ethyl alcohol, acetone, benzene, arene chloride.Use: This.. |
|||
Melting Point | 340 °C | 644 °F | ISO 11357 |
Quadrant EPP Ketron® CA30 LSG PEEK, Extruded 30% Carbon Fiber Reinforced Polyetherether Ketone (ASTM Product Data Sheet) |
|||
Melting Point | 340 °C | 644 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Ketron® CM GF30 Compression Molded, 30% Glass Reinforces Polyethererther Ketone(ASTM Product Data Sheet) |
|||
Melting Point | 340 °C | 644 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Ketron® CM HPV PEEK Polyetheretherketone; PTFE, Graphite, and Carbon Fiber Filled Bearing Grade, compression molded (ASTM Product Data Sheet) Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to hot water or steam |
|||
Melting Point | 340 °C | 644 °F | ASTM D3417 |
Quantum PEEK 30% Carbon Filled Information provided by Quantum Advanced Engineering Plastics |
|||
Melting Point | 340 °C | 644 °F | Peak (major component); ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been formula.. |
|||
Melting Point | 340 °C | 644 °F | Peak (major component); ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining most of.. |
|||
Melting Point | 340 °C | 644 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical prope.. |
|||
Melting Point | 340 °C | 644 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-820 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 NL is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire PEEK is produced to the highest industry standard.. |
|||
Melting Point | 340 °C | 644 °F | ASTM D3417 |
Solvay Specialty Polymers KetaSpire® KT-820FP Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820FP is the low-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color fine powder form suitable for compression molding. KetaSpire PEEK is produced to the .. |
|||
Melting Point | 340 °C | 644 °F | ASTM D3417 |
Solvay Specialty Polymers KetaSpire® KT-820P Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820P is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire PEEK is produced to the highest industry standards and is .. |
|||
Melting Point | >= 340 °C | >= 644 °F | ISO 3146 |
Panjin Zhongrun Chemerize 012G High Viscosity CoPEEK Information provided by Bieglo Gmbh. |
|||
Melting Point | 340 °C | 644 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Semitron® ESd 490HR Static dissipative PEEK for use in test fixtures. Non-sloughing and low moisture absorption. (ASTM Product Data Sheet) |
|||
Melting Point | 340 °C | 644 °F | ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621.. |
|||
Melting Point | 340 °C | 644 °F | ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK) AvaSpire® AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. .. |
|||
Melting Point | 340 °C | 644 °F | ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber KetaSpire® KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS.. |
|||
Melting Point | 340 °C | 644 °F | ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-820 NL Polyetheretherketone (PEEK) KetaSpire® KT-820 NL is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire® PEEK is produced to the highest industry .. |
|||
Melting Point | 340 °C | 644 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-820FP Polyetheretherketone (PEEK) KetaSpire® KT-820FP is the low-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color fine powder form suitable for compression molding. KetaSpire® PEEK is produced.. |
|||
Melting Point | 340 °C | 644 °F | ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK) KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula.. |
|||
Melting Point | 340 °C | 644 °F | DSC |
Wolf Kunststoff ZEDEX® ZX-324V2T A3F PEEK, PTFE Modified Reduced friction; High wear resistance; High elasticity; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automotive Technology; Machine ToolsInformation provided by Zedex |
|||
Melting Point | 340 °C | 644 °F | DSC |
Wolf Kunststoff ZEDEX® ZX-324VMT A3B PEEK, Fiber Reinforced Main Characteristics: Maximum rigidity; Very good wear resistance; Low stick-slip tendency; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInfor.. |
|||
Melting Point | 340 °C | 644 °F | ISO 1218 Method A; DIN 53736 |
Zell-Metall Engineering Plastics Zellamid 1500 (PEEK) Zellamid® 1500 (Polyetheretherketone - PEEK, natural) is the registered trademark for Zell-Metalls semi-crystalline high performance thermoplastic which exhibits a unique combination of high m.. |
|||
Melting Point | 340 °C | 644 °F | |
Ensinger Tecapeek® MT CF 30 Polyetheretherketone (PEEK) TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti.. |
|||
Melting Point | 340 °C | 644 °F | |
Ensinger Tecapeek® MT Polyetheretherketone (PEEK) TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti.. |
|||
Melting Point | 340 °C | 644 °F | |
Ensinger Tecapeek® Polyetheretherketone (PEEK) TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti.. |
|||
Melting Point | 340 °C | 644 °F | 10K/min; ISO 3146 |
CENTROPLAST CENTROPEEK Polyetheretherketone This plastic has high temperature resistance, good chemical resistance, and good mechanical characteristics. Its has good sliding friction properties and is suitable for use with foodstuffs or medi.. |
|||
Melting Point | 340 °C | 644 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. The .. |
|||
Melting Point | 340 °C | 644 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621 CF30 gr.. |
|||
Melting Point | 340 °C | 644 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This resin ret.. |
|||
Melting Point | 340 °C | 644 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical strength a.. |