Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.90 GPa | 856 ksi | ISO 527-1/-2 |
Quadrant EPP Ketron® HPV PEEK + carbon fibres + PTFE + graphite, bearing grade, extruded (ISO Data) The addition of carbon fibres, PTFE and graphite to virgin PEEK results in a Ketron PEEK “bearing grade”. Its excellent tribological properties (low friction, long wear and high pressure-velocity .. |
|||
Tensile Modulus | 5.90 GPa | 856 ksi | ISO 527-2 |
NOVA Chemicals DYLARK® 480P16 Glass Reinforced Engineering Resin Features:Very high modulus High heat resistance Excellent flow characteristics Excellent adhesion to urethaneApplications:Instrument panel substrates Consoles Cluster housings Interior trimInformati.. |
|||
Tensile Modulus | 5.90 GPa | 856 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Faradex EX06464 PEI (Asia Pacific) LNP* Faradex* EX06464 is a compound based on Polyetherimide resin containing Stainless Steel. Added features of this material include: Electrically
Conductive, EMI/RFI Shielding.This data was suppli.. |
|||
Tensile Modulus | 5.90 GPa | 856 ksi | |
Plastcom SLOVALEN PH 66 GF 30 FRO 4 PP, 30% glass fibre, mod. of mech. prop. Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Tensile Modulus | 5.90 GPa | 856 ksi | ISO 527 |
Nilit FRIANYL B63 MG30 Nylon 6 for injection molding, 30% mineral filled Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 5.90 GPa | 856 ksi | ASTM D638 |
PolyOne Edgetek® AS- 08CF / 000 ABS - 8% Carbon Fiber Reinforced With ESD Properties
(discontinued **) Data provided by PolyOne. |
|||
Tensile Modulus | 5.90 GPa | 856 ksi | ASTM D638 |
PolyOne Edgetek® AS-10CF/000 ABS - 10% Carbon Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Tensile Modulus | 5.90 GPa | 856 ksi | Dried; ISO 527 |
Manifattura Cattaneo PA 6.6 30% GF Nylon, Glass Filled Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Tensile Modulus | 5.90 GPa | 856 ksi | ISO 527-1,-2 |
Lanxess Durethan® AKV 15 H3.0 000000 Nylon 66, 15% Glass Fibers PA 66, 15% glass fibers, injection molding, heat-ageing stabilized |
|||
Tensile Modulus | 5.90 GPa | 856 ksi | 1 mm/min; ISO 527-1,-2 |
Lanxess Durethan® BKV 115 H2.0 DUS008 000000 Nylon 6, 15% Glass Fiber PA 6, 15% glass fibers, injection molding, impact modified, heat-ageing stabilizedInformation provided by LANXESS. |
|||
Tensile Modulus | 5.90 GPa | 856 ksi | ISO 527-1, -2; 1 mm/min |
Lanxess Pocan® B 3216 HR 000000 PBT 16% Glass Fiber PBT, 16% glass fibers, injection molding, improved impact strength, hydrolysis stabilizedInformation provided by LANXESS. |
|||
Tensile Modulus | 5.90 GPa | 856 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® BKV 30 H2.0 901510 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, good heat-ageing resistanceApplication Examples: pedal brackets, automotive front end structures |
|||
Tensile Modulus | 5.90 GPa | 856 ksi | |
LATI Latishield 66-10A G/15 PA66, Steel/Glass Fiber Reinforced EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Tensile Modulus | 5.90 GPa | 856 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp KFL34 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KFL34 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 5.90 GPa | 856 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP KZL16 Acetal Copolymer (Europe-Africa-Middle East) LNP* LUBRICOMP* KZL16 is a compound based on Acetal Copolymer resin containing milled Glass and PTFE. Added features include; Internally Lubricated. |
|||
Tensile Modulus | 5.90 GPa | 856 ksi | ISO 527 Type 1A |
Solvay TECHNYL® B 218L V30 Black 44 N PA66, 30% glass fiber, Conditioned Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding, heat stabilized with improved UV ageing resistance.Available in: Asia Pacific, Europe and Latin AmericaProdu.. |
|||
Tensile Modulus | 5.90 GPa | 856 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFL33 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFL33 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. |
|||
Tensile Modulus | 5.90 GPa @Temperature 150 °C |
856 ksi @Temperature 302 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Tensile Modulus | 5.90 GPa | 856 ksi | ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-820 GF13 Polyetheretherketone (PEEK), 13% Glass Fiber KetaSpire® KT-820 is a low flow, 13% glass fiber reinforced grade of polyetheretherketone (PEEK). The glass fiber content is optimized to provide a balance of strength and stiffness with toughnes.. |
|||
Tensile Modulus | 5.90 GPa | 856 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® DR51 PBT (Europe-Africa-Middle East) VALOX DR51 is a 15% glass fiber reinforced PBT injection moulding resin with excellent mechanical, thermal and electrical performance. Applications: spotlights, appliance housings, handles. |
|||
Tensile Modulus | 5.90 GPa | 856 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® VX5121 PBT (Europe-Africa-Middle East) VALOX VX5121 is a 15 % glass reinforced PBT+PC blend with low warpage characteristics.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 5.90 GPa | 856 ksi | ISO 527 |
Polyram RamLloy PB917G6 Nylon 6/Polypropylene Alloy, 30% Glass Fiber Reinforced 30% Glass fiber reinforced Nylon6/PP alloy with reduced water absorption, dimensional stability and UV stabilized, for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 5.90 GPa | 856 ksi | ISO 527-1/-2 |
Covestro Bayblend® T88-4N Polycarbonate + ABS, 20% Glass Filled Injection molding grade20 % glass fiber filledtensile modulus = 5900 MPaVicat/B 120 temperature = 134 °CPreprocessingMax. Water content |
|||
Tensile Modulus | 5.90 GPa | 856 ksi | cond.; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 GF30 I Polyamide 6 - Glass Fiber Reinforced 30% Glass fiber reinforced, impact modified, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following mai.. |
|||
Tensile Modulus | 5.90 GPa | 856 ksi | D638 |
Ascend Performance Materials VYDYNE® R220 Nylon, Mineral Reinforced Typical property data. VYDYNE is a registered trademark of Solutia Inc. |
|||
Tensile Modulus | 5.90 GPa | 856 ksi | ISO 527-2 |
CENTROPLAST CENTROMID 6.6 GF 30 Polyamide 6.6 30% glass fiber This material has very high strength and rigidity, with lower moisture absorption. It can be used for housing parts, threaded bolts, and distance pieces.Information provided by CENTROPLAST Engineer.. |
|||
Tensile Modulus | 5.90 GPa | 856 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Minlon® 11C40 NC010 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66 Minlon 11C40 NC010 is a 40% mineral reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 5.90 GPa | 856 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R860 BK02 Nylon 66, Glass/Mineral Reinforced, Conditioned Vydyne® R860 BK02 is general-purpose, glass-fiber and mineral-reinforced PA66 resin. Available in black, this product is also lubricated for improved flow and offers superior surface appearance. Gl.. |
|||
Tensile Modulus | 5.90 GPa | 856 ksi | ASTM D638 |
PolyOne Lubri-Tech™ MP-30GF/15T Modified PPO - 30% Glass Fiber - 15% PTFE
(discontinued **) Data provided by PolyOne. |