Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.660 MPa-m/sec
18800 psi-ft/min
at 0.1 m/s unlubricated
Quadrant EPP Ketron® HPV PEEK + carbon fibres + PTFE + graphite, bearing grade, extruded (ISO Data)
The addition of carbon fibres, PTFE and graphite to virgin PEEK results in a Ketron PEEK “bearing grade”. Its excellent tribological properties (low friction, long wear and high pressure-velocity ..
Limiting Pressure Velocity 0.660 MPa-m/sec
18800 psi-ft/min
at 0.1 m/s unlubricated
Quadrant EPP Ketron® TX PEEK + solid lubricant, extruded (ISO Data)
This member of the Ketron PEEK family has been developed especially for the food industry. Like Ketron PEEK-1000, this new internally lubricated material has a food contact compliant composition, bu..