Thermal Properties Metric English Comments
Thermal Conductivity 0.780 W/m-K
5.41 BTU-in/hr-ft²-°F
Quadrant EPP Ketron® HPV PEEK + carbon fibres + PTFE + graphite, bearing grade, extruded (ISO Data)
The addition of carbon fibres, PTFE and graphite to virgin PEEK results in a Ketron PEEK “bearing grade”. Its excellent tribological properties (low friction, long wear and high pressure-velocity ..
Thermal Conductivity 0.780 W/m-K
5.41 BTU-in/hr-ft²-°F
Schott F2 Glass
Information Provided by SCHOTT North America, Inc.
Thermal Conductivity 0.780 W/m-K
5.41 BTU-in/hr-ft²-°F
Schott F2HT Glass
Information Provided by SCHOTT North America, Inc.
Thermal Conductivity 0.780 W/m-K
5.41 BTU-in/hr-ft²-°F
Schott N-BAF10 Glass
Information Provided by SCHOTT North America, Inc.
Thermal Conductivity 0.780 W/m-K
5.41 BTU-in/hr-ft²-°F
Moulding Direction; ASTM C177
Dalau Dalcon 018 85% Virgin PTFE, 15% Graphite
Applications & Industries: General: Graphite filler improves the sliding properties & thermal conductivity of PTFE and has one of the lowest coefficient of frictions. It has low wear in water and is..
Thermal Conductivity 0.780 W/m-K

@Temperature 121 °C
5.41 BTU-in/hr-ft²-°F

@Temperature 250 °F
Tra-Con Tra-Bond 342-14T Low Viscosity Room Temperature Cure Epoxy Adhesive
TRA-BOND 342-14T single component, low viscosity alumina-filled epoxy adhesive exhibits high bond strength and excellent thermal shock characteristics. This adhesive may be cured at room temperature..
Thermal Conductivity 0.780 W/m-K
5.41 BTU-in/hr-ft²-°F
Moulding Direction; ASTM C177
Dalau Dalcon 018 85% Virgin PTFE, 15% Graphite
Applications & Industries: General: Graphite filler improves the sliding properties & thermal conductivity of PTFE and has one of the lowest coefficient of frictions. It has low wear in water and is..
Thermal Conductivity 0.780 W/m-K

@Temperature 50.0 °C
5.41 BTU-in/hr-ft²-°F

@Temperature 122 °F
3M XLD3000 Glass Bubbles
3M™ Glass Bubbles XLD3000 are high-strength additives for polymers made from a water-resistant and chemically stable soda-lime-borosilicate glass. These hollow glass bubbles can be compounded with ..