Plastcom PLASTAMID® 6 BT N 26 B/IM PA6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer Plastcom spol. s r.o.
Trade Name PLASTAMID®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom PLASTAMID® 6 BT N 26 B/IM PA6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Basic type PA 6 for injection molding, for general use. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, clamps, hobby tools. Delivered in the natural mode and in the full RAL color scale.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
STN EN ISO 1183-1
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 230 °C
25 g/10 min

@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 75.0 MPa
10900 psi
STN EN ISO 527-2
Elongation at Break 3.5 %
3.5 %
STN EN ISO 527-2
Tensile Modulus 2.00 GPa
290 ksi
STN EN ISO 527-2
Flexural Strength 85.0 MPa
12300 psi
STN EN ISO 178
Flexural Modulus 2.00 GPa
290 ksi
STN EN ISO 178
Charpy Impact Unnotched 5.00 J/cm²

@Temperature -20.0 °C
23.8 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
7.00 J/cm²

@Temperature 23.0 °C
33.3 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Charpy Impact, Notched 0.150 J/cm²

@Temperature 23.0 °C
0.714 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
0.150 J/cm²

@Temperature -20.0 °C
0.714 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
STN EN 11357-1
Processing Properties Metric English Comments
Melt Temperature 260 - 290 °C
500 - 554 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 80.0 °C

@Time 14400 sec
176 °F

@Time 4.00 hour
Moisture Content 0.20 %
0.20 %
STN EN ISO 3344
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi