Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 85.0 MPa | 12300 psi | STN EN ISO 178 |
Plastcom PLASTAMID® 6 BT N 26 B/IM PA6 Basic type PA 6 for injection molding, for general use. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, clamps, hobby tools. Delivered in the natu.. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | |
Poco Graphite DFP Semiconductor Grade Graphite Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their .. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | ISO 178 |
Polycasa XT 620 PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
Flexural Strength | <= 85.0 MPa | <= 12300 psi | ISO 178 |
Polykemi AB POLYshine PBT D223 Q30 FR PBT, Mineral Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Flexural Strength | 85.0 MPa @Temperature 23.0 °C |
12300 psi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Crastin® S600F20 NC010 PBT
(Unverified Data**) Crastin® S600F20 NC010 is an unreinforced, lubricated, medium viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Strength | 85.0 MPa | 12300 psi | ISO 178 |
Polycasa COPOL PETG QUINN COPOL has good optical properties, brilliant surface, easy to vacuum form without pre-drying, low water absorption, very good chemical resistance, and high impact properties.Bus shelters (UV-v.. |
|||
Flexural Strength | <= 85.0 MPa | <= 12300 psi | ISO 178 |
Polykemi AB POLYabs HH0 ABS, Extra Heat Resistance Information provided by Polykemi AB |
|||
Flexural Strength | 85.0 MPa | 12300 psi | ASTM D790M |
DSM Somos® 7110 Epoxy Photopolymer, UV Postcure
(discontinued **) DescriptionDSM Somos® 7110 Photopolymer is a humidity-tolerant, high heat-deflection-temperature, low-curl, high-speed liquid that produces rigid, highly accurate parts. It produces exceptional, u.. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
Hexion Bakelite™ PF 85 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, organically filled, reinforced with cotton fibers, average notched impact strength, UL listed molding compound 1.5 mm/HB (BK, BN).Application areas: Switch covers, rolls, .. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | |
Lehmann & Voss LUVOCOM® 1105-8319 PEEK, with PTFE, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts.Improved friction and wear behaviour. Emergency r.. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | 2mm/min; ASTM D790 |
Kingfa JH830T Flame Retardant PC Features:UL V-0 @ 2.4mmExcellent balance propertiesHigh stiffnessGood size stabilityGood surfaceTransparentApplications:Controller switchLamp-chimneyTelecommunicationHousehold appliance cabinetInfor.. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | 2mm/min; ASTM D790 |
Kingfa JH960 6100 Non-halogenated Flame Retardant PC/ABS Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent mechanical propertiesChemical resistanceHydrolysis resistanceDrop down resistantSuper high flow ability, suit for thin w.. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | ASTM D790 |
LG Chemical HI835S PMMA, Impact Resistant Grade Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che.. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | 2mm/min; ASTM D790 |
Kingfa PC-S923 Modified PC Features:Excellent balance propertiesGood weather resistanceHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelElec.. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | ASTM D790 |
Kotec Carbotex K-20UV Polycarbonate, General Purpose, UV Stability Grade Features: UV Stability, High flow, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting Covers, Safety products, E & E parts, Household applications, Leisure.. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | ASTM D790 |
Kotec Carbotex K-30UVR Polycarbonate, General Purpose, UV Stability + Mold Release Grade Features: UV stability, Mold release, Medium viscosityApplications: OA equipment, Communications, Precision parts, Machineries, Lighting fixtures/covers, Safety products, E & E parts, Household appl.. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | ISO 178 |
Mitsubishi Xantar® C CM 506 U Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | 1.3 mm/min; ASTM D790 |
Lavergne VYPET VNT 1021 Polyester-PC Alloy The Vypet 1021 Black is a medium viscosity Polyester and PC alloy, has an excellent balance of stiffness and impact resistance.Features: Excellent Processability; Good Impact Resistance; Good Chemic.. |
|||
Flexural Strength | 85.0 MPa @Strain 6.00 % |
12300 psi @Strain 6.00 % |
2 mm/min; ISO 178-A |
Lanxess Pocan® B 1701 000000 PBT PBT, non-reinforced, extrusion, food contactInformation provided by LANXESS. |
|||
Flexural Strength | 85.0 - 135 MPa | 12300 - 19600 psi | |
Schott Dark ROBAX® Glass Ceramic Dark ROBAX® is an infra-red transparent glass-ceramic having virtually zero thermal expansion and sufficient mechanical resistance required for all standard applications. It is produced in rolle.. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RP003 PA 66 (Asia Pacific) LNP* Lubricomp* RP003 is a compound based on Nylon 66 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | ISO 178 |
Styrolution Terblend® N NG-02 EF 8% Glass Filled ABS+PA (Dry) Description: Terblend® N NG-02 EF is a glass fiber reinforced UV stabilized ABS/PA blend with excellent dimensional stability and high impact strength. The enhanced flowability enables excellent .. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | 1 mm/min; ISO 178 |
Styron Pulse® A35-110 PC/ABS PULSE™ A35-110 engineering resins give exceptional impact strength even at low temperatures and have high heat distortion temperature. The proprietary mass ABS technology of Dow allows these p.. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP WZ002 PBT LNP* THERMOCOMP* WZ002 is a compound based on PBT resin containing 10% Milled Glass. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1602 Glass Reinforced, Chemically Coupled Homopolymer DescriptionPolyfort® FPP 1602 is a 10% glass reinforced chemically coupled homopolymer.Information provided by A. Schulman. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | ASTM D790 |
Plenco 4300 Phenolic, Granular, Injection Molded PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electric.. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | ISO 178 |
DuPont Performance Polymers Crastin® FG6134 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced Medium Viscosity Polybutylene Terephthalate Developed for Food Contact Applications Crastin® FG6134 NC010 is an unreinforced medium viscosity polybutylene terephthalate resin for injec.. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | ISO 178 |
DuPont Performance Polymers Crastin® S600F40 BK851 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Low Viscosity Polybutylene Terephthalate Crastin S600F40 BK851 is an unreinforced lubricated low viscosity black polybutylene terephthalate resin for injection molding.Information provi.. |
|||
Flexural Strength | 85.0 MPa @Temperature 120 °C |
12300 psi @Temperature 248 °F |
ASTM Test |
BASF Petra® 130 30% Glass Filled PET Petra 130 is a 30% glass fiber reinforced polyethylene terephthalate (PET) for injection molding applications. It exhibits a good combination of performance properties including high strength and s.. |
|||
Flexural Strength | 85.0 MPa | 12300 psi | ISO 178 |
BASF Ultradur B 6550 PBT Ultradur B 6550 is a high viscosity PBT extrusion grade.Applications; Used for loose buffer tubes for optical fibers, semi-finished products fro machining, profiles and pipes. |