Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 7.00 J/cm² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 6 BT N 26 B/IM PA6 Basic type PA 6 for injection molding, for general use. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, clamps, hobby tools. Delivered in the natu.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® A ECP3808 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® LM70G35HSLX BK314 Nylon 66
(Unverified Data**) Zytel® LM70G35HSLX is a 35% glass fiber reinforced, heat stabilized, lubricated polyamide 66 for injection molding. It is well suited for laser marking.Information provided by DuPont Performance Po.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® K224-HG5 (Dry) 25% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® K230-HXG6 Nylon 6-30% Glass Reinforced (European Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature 600 °C |
33.3 ft-lb/in² @Temperature 1110 °F |
|
Kennametal Stellite Nucalloy® 488 High-Silicon Nickel-Base Hardfacing Alloy Nucalloy® alloys are unique, patented, high-silicon, nickel-base hardfacing alloys that are designed to have optimum combinations of hardness and toughness, similar to the cobalt base alloys . B.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Durethan® AKV 30 G H2.0 SR1 900051 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, better surface than AKV 30 H2.0, good heat-ageing resistance |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 179/1eU |
Lanxess Durethan® BKV 130 GIT 900116 Copolyamide, 30% Glass Fiber CoPA, injection molding grade, 30% glass fibers, elastomer-modified, suitable for GIT (gas assisted technology), good surface finishApplication Examples: Chain-saw handles, office chair armrests, of.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 179-1eU |
Lanxess Durethan® BKV 215 H2.0 DUS008 901510 Nylon 6, Impact Modified PA 6, 15% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 179/1eU |
Lanxess Durethan® BKV 30 000000 Nylon 6, 30% Glass Fiber 30% Glass fiber reinforced; injection molding grade |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Durethan® BKV 35 H2.0 EF 900116 Nylon 6, 35% Glass Fiber PA 6, injection molding grade, 35% glass fibers, good heat-ageing resistance, good flowability (easy flow) |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Durethan® BKV 30 H2.0 901510 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, good heat-ageing resistanceApplication Examples: pedal brackets, automotive front end structures |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® K224-G6 (Cond.) 30% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® K224-HG6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® S223-G4U (Cond.) 23% Glass Reinforced Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® S223-HG6 (Cond.) 30% Glass Reinforced Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® S223-HG6 Nylon 66-30% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179/eU |
Eurotec® Tecodur® PB70 GR20 NL IH PBT 20% glass fiber reinforced, impact modified Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Akro-Plastic Akromid® B3 GF 50 RM-M (3146) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultraform® N2520 L POM Description: Is a POM, product having reduced electric surface resistance.Information provided by BASF |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Ascend Performance Materials Vydyne® R533H NT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H NT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties .. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Akro-Plastic Akromid® B3 GF 30 9 RM-M (3099) PA 6 Dry, 30% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Akro-Plastic Akromid® B3 GF 30 RM-M (3016) PA 6 Dry, 30% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Akro-Plastic Akromid® B3 GF 50 9 RM-M (3147) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Akro-Plastic Akromid® T6 GF 40 (3500) PPA Dry, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Ascend Performance Materials Vydyne® R533H BK0201 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK0201 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80x10x4mm; ISO 179/1eU |
SYNTHOS Krasten® 336M High Impact Polystyrene Easy flow grade. Processed by injection moulding of intricate and thin-walled products that enables high production output.Synthos was formerly known as Kaucuk. All information provided by Synthos. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 179/1eU |
Lanxess Durethan® BKV 30 W1 000000 Nylon 6, 30% Glass Fiber PA 6, Injection molding grade, 30% glass fibers, weather stabilized |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Durethan® DP AKV 35 LT H2.0 904040 Nylon 66, 35% Glass Fiber PA 66, injection molding grade, 35% glass fibers, black colored for laser transmission- welding (laser-transparent), good heat-ageing resistance |